VESTAMID® NRG 4101 yellow

Category: Nylon 12 , Polyamide 12
Manufacturer: Evonik Industries AG
Trademark: VESTAMID® NRG
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: nRBWiv_VESTAMID-NRG-4101-yellow.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
For Steel Pipe Protection (Encasement)

VESTAMID® NRG 4101 offers a flexible, mechanically tough encasement system that combines the advantages of polyethylene coating and cement mortar casing.

Uses of VESTAMID® NRG Products:
The important advantages of VESTAMID® NRG 4101 as an encasement material are:
  • unusually high impact resistance and toughness, even at low temperatures
  • excellent stress cracking resistance
  • excellent wear resistance
  • low sliding friction coefficient
Product characteristics compared with other encasement materials:
VESTAMID® NRG 4101 yellow has higher Shore hardness than polyethylene or polypropylene. In contrast to polyethylene or propylene encasement, therefore, the polyamide encasement offers, apart from the corrosion protection provided by the barrier effect, also mechanical protection for the encased steel pipe.

Application areas for the new encasement material are found in non-conventional installation technologies such as:
  • horizontal directional drilling
  • the soil displacement method with non-steered displacement hammers
  • dynamic ramming
  • plow technology

We recommend a processing temperature between 230°C (446°F) and 260°C (500°F) - in some cases up to 280°C (536°F) - during the extrusion process.

Drying at 80°C (176°F) for 2 hours to 4 hours before processing is recommended.
General Information
Features
  • Durable
  • Good Toughness
  • High Molecular Weight
  • Hydrocarbon Resistant
Appearance
  • Yellow
Processing Method
  • Extrusion
PhysicalNominal ValueUnitTest Method
Density (23°C)1.02g/cm³ISO 1183
HardnessNominal ValueUnitTest Method
Shore Hardness (Shore D)73ISO 868
Ball Indentation Hardness 176.0MPaISO 2039-1
MechanicalNominal ValueUnitTest Method
Tensile Modulus 1350MPaISO 527-2
Tensile Stress (Yield)40.0MPaISO 527-2
Tensile Strain ISO 527-2
    Yield 12%
    Break > 150%
ImpactNominal ValueUnitTest Method
Charpy Unnotched Impact Strength (-40°C)No BreakISO 179/1eU
ThermalNominal ValueUnitTest Method
Vicat Softening Temperature 170°CISO 306/A
Melting Temperature 2177°CISO 11357-3
ExtrusionNominal ValueUnit
Drying Temperature 80.0°C
Drying Time 2.0 to 4.0hr
Melt Temperature 230 to 280°C
Note Message
1 .H30
2 .2nd Heating
Resin Grade Manufacturer Category Trademark
Unipren® Elastomers B3 PRTA010 70A EG06S1 UP341 Petropol Industry and Trade of Polymers LTDA PP+EPDM Unipren® Elastomers
FLEXAREN® 18002 Innospec Leuna GmbH EVA FLEXAREN®
FLEXITEQ™ F60A111UV Marplex Australia Pty. Ltd. TPV FLEXITEQ™
KPOL-LLDPE LL K-1.1/918 KPOL Chem Co. LLDPE KPOL-LLDPE
Sylvin 4299-60 Natural Sylvin Technologies Incorporated PVC, Unspecified Sylvin