KOPA® KN173HI3R

Category: Nylon 6 , Polyamide 6
Manufacturer: Kolon Plastics, Inc.
Trademark: KOPA®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: mfGyWG_KOPA-KN173HI3R.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
KOPA® KN173HI3R is a Polyamide 6 (Nylon 6) product. It can be processed by extrusion and is available in Asia Pacific, Europe, Latin America, or North America.

Characteristics include:
  • Flame Rated
  • High Viscosity
  • Impact Resistant
General Information
Features
  • Good Impact Resistance
  • High Viscosity
Forms
  • Pellets
Processing Method
  • Extrusion
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.09g/cm³ASTM D792
Molding Shrinkage - Flow 1.3 to 1.6%ASTM D955
Water Absorption (Equilibrium, 23°C, 60% RH)1.1%ASTM D570
HardnessNominal ValueUnitTest Method
Rockwell Hardness (R-Scale)110ASTM D785
MechanicalNominal ValueUnitTest Method
Tensile Strength (Yield, 23°C)59.0MPaASTM D638
Tensile Elongation (Yield, 23°C)250%ASTM D638
Flexural Modulus (23°C)2060MPaASTM D790
Flexural Strength (23°C)88.0MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (23°C)250J/mASTM D256
ThermalNominal ValueUnitTest Method
Deflection Temperature Under Load ASTM D648
    0.45 MPa, Unannealed 160°C
    1.8 MPa, Unannealed 65.0°C
Melting Temperature 215°CASTM D1525
CLTE - Flow 1.0E-4cm/cm/°CASTM D696
ElectricalNominal ValueUnitTest Method
Dielectric Strength 20kV/mmASTM D149
Dielectric Constant (1 MHz)3.20ASTM D150
Arc Resistance 125secASTM D495
FlammabilityNominal ValueUnitTest Method
Flame Rating HBUL 94
Resin Grade Manufacturer Category Trademark
RTP 400 HI RTP Company PS (HIPS) RTP
TAROMID A 280 G3 X0 Taro Plast S.p.A. Nylon 66 TAROMID A
Ultramid® A3WGM33 BK20560 BASF Corporation Nylon 66 Ultramid®
Varcum 29202 Durez Corporation Phenolic Varcum
POLIMAXX 1202J IRPC Public Company Limited PP Homopolymer POLIMAXX