Category: | TPU-Polyether , Thermoplastic Polyurethane Elastomer (Polyether) |
Manufacturer: | BASF Polyurethanes GmbH |
Trademark: | Elastollan® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | mFbkfW_Elastollan-1174-D.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms. Typical applications Cable jackets, plugs and terminations, spiral tubing, Films, ski-boot shells, ear tags, technical mouldings like mining screens, railway pads, seals. |
General Information | |
---|---|
Features |
|
Uses |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.20 | g/cm³ | ISO 1183/A |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Shore Hardness (Shore D, 3 sec) | 73 | ISO 7619 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 560 | MPa | ISO 527-2 |
Abrasion Loss | 20.0 | mm³ | ISO 4649-A |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | DIN 53504 | ||
20% Strain | 25.0 | MPa | |
100% Strain | 30.0 | MPa | |
300% Strain | 45.0 | MPa | |
Tensile Stress | DIN 53504 | ||
Yield 1 | 35.0 | MPa | |
Yield | 50.0 | MPa | |
Tensile Elongation | DIN 53504 | ||
Break 2 | 400 | % | |
Break | 300 | % | |
Tear Strength 3 | 220 | kN/m | ISO 34-1 |
Compression Set | ISO 815 | ||
23°C, 72 hr | 50 | % | |
70°C, 24 hr | 55 | % |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | ||
-30°C | 5.0 | kJ/m² | |
23°C | No Break |
Injection | Nominal Value | Unit | |
---|---|---|---|
Processing (Melt) Temp | 170 to 240 | °C | |
Mold Temperature | 20.0 to 70.0 | °C |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Melt Temperature | 160 to 220 | °C |
Note Message | |
---|---|
1 . | after storage in water at 80°C for 42 days |
2 . | after storage in water at 80°C for 42 days |
3 . | Method Bb, Angle (Nicked) |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Vydyne® 47 | Ascend Performance Materials Operations LLC | Nylon 66 | Vydyne® |
Complet® LCF40-PA6 | PlastiComp, Inc. | Nylon 6 | Complet® |
ELASTOSIL® R plus 4110/60 | Wacker Chemie AG | Silicone | ELASTOSIL® R plus |
Sylvin 2946-75 White 1547 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
SABIC® LDPE PCG01 | Saudi Basic Industries Corporation (SABIC) | LDPE | SABIC® LDPE |