| Category: | Nylon, Unspecified , Polyamide |
| Manufacturer: | Teknor Apex Company (Chem Polymer) |
| Trademark: | Chemlon® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | mA9ylR_Chemlon90413GVNH.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Chemlon®904-13 GVNH is a polyamide material,. This product is available in North America,. Chemlon®The main characteristics of 904-13 GVNH are: flame retardant/rated flame. Chemlon®The typical application fields of 904-13 GVNH are: automobile industry |
| General Information | |
|---|---|
| Uses |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density (23°C) | 1.31 | g/cm³ | ISO 1183 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus (23°C) | 6000 | MPa | ISO 527-2/1 |
| Tensile Stress (Yield) | 105 | MPa | ISO 527-2 |
| Nominal Tensile Strain at Break | 3.0 | % | ISO 527-2 |
| Flexural Modulus | 5900 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179 | ||
| -30°C | 3.7 | kJ/m² | ISO 179 |
| 23°C | 4.5 | kJ/m² | ISO 179 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 245 | °C | ISO 75-2/A |
| Flammability | Nominal Value | Test Method | |
|---|---|---|---|
| Flame Rating (0.8 mm) | V-0 | UL 94 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Shin-Etsu Elastomer KE-2004-5A/B | Shin-Etsu Silicones of America | Silicone Rubber, HTV | Shin-Etsu Elastomer |
| Arnitel® EM740 | DSM Engineering Plastics | TPC-ET | Arnitel® |
| ELASTOSIL® LR 3003/20 TR A/B | Wacker Chemie AG | Silicone | ELASTOSIL® LR |
| Hostacom X M1 T06 | LyondellBasell Industries | PP Copolymer | Hostacom |
| IROGRAN® A 78 E 4723 | Huntsman Corporation | TPU-Polyester | IROGRAN® |