Category: | PBT , Polybutylene Terephthalate |
Manufacturer: | PolyOne Corporation |
Trademark: | Bergadur™ |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | lKcsIO_BergadurPB40G20.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Bergadur™PB40 G20 is a polybutene terephthalate (PBT) product, which contains a 20% glass fiber reinforced material. It can be processed by injection molding and is available in Europe. |
General Information | |
---|---|
Filler / Reinforcement |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.46 | g/cm³ | ISO 1183 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 6700 | MPa | ISO 527-2 |
Tensile Stress | 105 | MPa | ISO 527-2 |
Tensile Strain (Break) | 3.0 | % | ISO 527-2 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | ||
-30°C | 7.0 | kJ/m² | ISO 179 |
23°C | 8.0 | kJ/m² | ISO 179 |
Charpy Unnotched Impact Strength | ISO 179 | ||
-30°C | 35 | kJ/m² | ISO 179 |
23°C | 40 | kJ/m² | ISO 179 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 110 - 130 | °C | |
Drying Time | 4.0 - 6.0 | hr | |
Rear Temperature | 240 - 270 | °C | |
Middle Temperature | 240 - 270 | °C | |
Front Temperature | 240 - 270 | °C | |
Mold Temperature | 75 - 95 | °C |
Injection instructions |
---|
Injection Pressure: MED-HIGHHold Pressure: MED-HIGHScrew Speed: MODERATEBack Pressure: LOW |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
VENELENE® FD-0325 | Poliolefinas Internacionales, C.A. (Polinter) | LDPE | VENELENE® |
Niretan A F50 | Soredi S.p.a. | Nylon 66 | Niretan A |
GAPEX® RPP20EU04NA | Ferro Corporation | PP, Unspecified | GAPEX® |
Grilon® BK-30 | EMS-GRIVORY | Nylon 6 | Grilon® |
Sylvin 4222-90LG Natural Dry Blend | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |