Category: | Silicone Rubber, LSR , Silicone Rubber, LSR |
Manufacturer: | Momentive Performance Materials Inc. |
Trademark: | LIM™ |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | k4xGGL_LIM-8040.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
LIM8040 liquid silicone rubber is a 2-component liquid injection moulding material, which offers primerless adhesion to a wide range of substrates including metals and engineering plastics. Full bond strength is reached immediately after de-moulding. This makes LIM 8040 the optimal choice for cost-efficient manufacturing of high numbers of articles in integrated processes such as multicomponent injection moulding or insert-moulding. If properly processed, parts made from LIM 8040 can meet the requirements for food contact. The requirements are determined in 21CFR FDA paragraph 177.2600 'Rubber articles intended for repeated use. It also has been successfully tested for USP class VI. Both applications usually require a postcure. Key Features and Benefits
Potential Applications LIM 8040 is particularly suitable for the manufacturing of parts, where engineering plastics and elastomeric materials need to be combined in an overmolding or co-molding process such as:
|
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
Forms |
|
Processing Method |
|
Thermal | Nominal Value | Unit | |
---|---|---|---|
Thermal Conductivity 1 | 0.19 | W/m/K |
Uncured Properties | Nominal Value | Unit | |
---|---|---|---|
Color | |||
-- 2 | Translucent | ||
-- 3 | Translucent | ||
Density | |||
-- 4 | 1.08 | g/cm³ | |
-- 5 | 1.08 | g/cm³ | |
Pot Life (20°C) | 4300 | min |
Cured Properties | Nominal Value | Unit | |
---|---|---|---|
Shore Hardness | |||
Shore A 6 | 43 | ||
Shore A 7 | 46 | ||
Tensile Modulus | |||
100% Secant 8 | 1.20 | MPa | |
100% Secant 9 | 1.60 | MPa | |
Tensile Strength | |||
-- 10 | 5.20 | MPa | |
-- 11 | 5.60 | MPa | |
Tensile Elongation at Break | |||
-- 12 | 380 | % | |
-- 13 | 390 | % | |
Compression Set | |||
150°C, 168 hr 14 | 27 | % | |
150°C, 1000 hr 15 | 35 | % | |
150°C, 168 hr 16 | 67 | % | |
150°C, 1000 hr 17 | 76 | % | |
Tear Strength | |||
Die B 18 | 30.2 | kN/m | |
Die B 19 | 37.8 | kN/m | |
Electric Strength | |||
-- 20 | 20 | kV/mm | |
-- 21 | 20 | kV/mm | |
Relative Permittivity | |||
-- 22 | 2.85 | ||
-- 23 | 2.85 | ||
Volume Resistivity | |||
-- 24 | 2.9E+14 | ohms·cm | |
-- 25 | 2.9E+14 | ohms·cm | |
Dissipation Factor | |||
-- 26 | 3.0E-3 | ||
-- 27 | 3.0E-3 |
Note Message | |
---|---|
1 . | Postbaked 1 hr @ 177°C (350°F) |
2 . | Part B |
3 . | Part A |
4 . | Part B |
5 . | Part A |
6 . | As Molded 30 sec @ 177°C (350°F) |
7 . | Postbaked 1 hr @ 177°C (350°F) |
8 . | As Molded 30 sec @ 177°C (350°F) |
9 . | Postbaked 1 hr @ 177°C (350°F) |
10 . | As Molded 30 sec @ 177°C (350°F) |
11 . | Postbaked 1 hr @ 177°C (350°F) |
12 . | Postbaked 1 hr @ 177°C (350°F) |
13 . | As Molded 30 sec @ 177°C (350°F) |
14 . | Postbaked 1 hr @ 177°C (350°F) |
15 . | Postbaked 1 hr @ 177°C (350°F) |
16 . | As Molded 30 sec @ 177°C (350°F) |
17 . | As Molded 30 sec @ 177°C (350°F) |
18 . | Postbaked 1 hr @ 177°C (350°F) |
19 . | As Molded 30 sec @ 177°C (350°F) |
20 . | Postbaked 1 hr @ 177°C (350°F) |
21 . | As Molded 30 sec @ 177°C (350°F) |
22 . | Postbaked 1 hr @ 177°C (350°F) |
23 . | As Molded 30 sec @ 177°C (350°F) |
24 . | Postbaked 1 hr @ 177°C (350°F) |
25 . | As Molded 30 sec @ 177°C (350°F) |
26 . | Postbaked 1 hr @ 177°C (350°F) |
27 . | As Molded 30 sec @ 177°C (350°F) |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Andur 7-3 APLF/Curene® 442 | Anderson Development Company | PUR-Ester/TDI | Andur |
Aplax P2313CN | Ginar Technology Co., LTD. | PP, Unspecified | Aplax |
Jampilen SP179 | Jam Polypropylene Company | PP Copolymer | Jampilen |
PLEXIGLAS® Sheet XT, UV transmitting Clear 0A770 | Evonik Industries AG | Acrylic (PMMA) | PLEXIGLAS® Sheet |
LNP™ LUBRICOMP™ SCL36 compound | SABIC Innovative Plastics | Nylon 12 | LNP™ LUBRICOMP™ |