Monprene PC-13970 XRD1 is a high performance thermoplastic elastomer, available in NAT and colors, designed for a variety of personal care consumer product applications requiring a soft, rubber-like feel, including toothbrush articles. Monprene PC-13970 XRD1 is a medium hardness, medium density, UV stabilized grade that complies with various US FDA and European regulations and directives for food contact and is suitable for injection molding. |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.05 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 12 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness | |||
Shaw A, 1 sec | 72 | ASTM D2240 | |
Shaw A, 5 seconds | 70 | ISO 868 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ISO 37 | ||
100% strain | 2.30 | MPa | ISO 37 |
300% strain | 2.40 | MPa | ISO 37 |
Tensile Strength (Break) | 8.30 | MPa | ISO 37 |
Tensile Elongation (Break) | 700 | % | ISO 37 |
Compression Set 1 | ISO 815 | ||
23°C, 22 hr | 34 | % | ISO 815 |
70°C, 22 hr | 55 | % | ISO 815 |
Fill Analysis | Nominal Value | Unit | Test Method |
---|---|---|---|
Apparent Viscosity (200°C, 206 sec^-1) | 110 | Pa·s | ISO 11443 |
Legal statement |
---|
The information and recommendations contained in this bulletin are, to the best of our knowledge, accurate and reliable but no guarantee of their accuracy is made. All products are sold upon condition that purchasers shall make their own tests to determine the suitability of such products for their particular purposes and uses and purchaser assumes all risks and liability for the results of use of the products, including use in accordance with seller's recommendations. Nothing in this bulletin constitutes permission or a recommendation to practice or use any invention covered by any patent owned by this company or others. There is no warranty of merchantability and there are no other warranties for the products described. For detailed Product Stewardship information, please contact us. Any product of Teknor Apex, including product names, shall not be used or tested in medical or food contact applications without the prior written acknowledgement of Teknor Apex as to the intended use. Please note that some products may not be available in one or more countries. |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 120 - 160 | °C | |
Middle Temperature | 160 - 230 | °C | |
Front Temperature | 180 - 230 | °C | |
Nozzle Temperature | 180 - 230 | °C | |
Processing (Melt) Temp | 180 - 230 | °C | |
Mold Temperature | 15 - 50 | °C | |
Injection Rate | Fast | ||
Back Pressure | 0.500 - 1.50 | MPa | |
Screw Speed | 50 - 100 | rpm | |
Cushion | 3.00 - 20.0 | mm |
Injection instructions |
---|
Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C). |
Note Message | |
---|---|
1 . | Method B |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Makrolon® ET IR320 | Covestro - Polycarbonates | PC | Makrolon® |
Synres® SR-1209A | Teknor Apex Company | PP, Unspecified | Synres® |
TOPAS® 8007F-600 | Topas Advanced Polymers, Inc. | COC | TOPAS® |
COSMOTHENE® EVA K3212 | TPC, The Polyolefin Company (Singapore) Pte Ltd | EVA | COSMOTHENE® EVA |
Sumiliteresin® PR-54529 | SBHPP | Phenolic | Sumiliteresin® |