| Category: | ABS , Acrylonitrile Butadiene Styrene |
| Manufacturer: | TER HELL PLASTIC GMBH |
| Trademark: | TEREZ ABS |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | icwmUp_TEREZ-ABS-3016.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Easy flowing ABS with good impact resistance. For moulding parts with low wall thickness and/or unfavourable flow distance/wall thickness relation. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.04 | g/cm³ | ISO 1183 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 2300 | MPa | ISO 527-2 |
| Tensile Stress (Yield) | 45.0 | MPa | ISO 527-2 |
| Tensile Strain | ISO 527-2 | ||
| Yield | 2.4 | % | |
| Break | 12 | % |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179/1eA | ||
| -30°C | 7.0 | kJ/m² | |
| 23°C | 19 | kJ/m² | |
| Charpy Unnotched Impact Strength (23°C) | 140 | kJ/m² | ISO 179/1eU |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature | |||
| 0.45 MPa, Unannealed | 90.0 | °C | ISO 75-2/B |
| 1.8 MPa, Unannealed | 78.0 | °C | ISO 75-2/A |
| Vicat Softening Temperature | 95.0 | °C | ISO 306/B50 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Advanced Composites ATX913-2 | Advanced Composites, Inc. | PP, Unspecified | Advanced Composites |
| CONTINUUM™ DGDA-2490 BK | The Dow Chemical Company | HDPE | CONTINUUM™ |
| Eco Cool Plus MP10 | EcolBiotech Co., Ltd | PLA | Eco Cool Plus |
| Edgetek™ AT-30GF/000 BK004 | PolyOne Corporation | Acetal (POM) Copolymer | Edgetek™ |
| Latamid 66 B H-V0 | LATI S.p.A. | Nylon 66 | Latamid |