HX-064AB is a fully-crosslinked thermoplastic elastomer(TPE) product. TPEs can be easily processed with general thermoplastic processing equipments. It has low compression set, good weatherability and excellent resistance to high temperature, chemicals, and ozone. Flexible PVC, rubbers (CR, NBR, EPDM etc.) can be replaced with TPE. |
General Information | |
---|---|
Features |
|
Uses |
|
RoHS Compliance |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.970 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A) | 70 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (100% Strain) | 3.43 | MPa | ASTM D412 |
Tensile Strength (Break) | 7.55 | MPa | ASTM D412 |
Tensile Elongation (Break) | 530 | % | ASTM D412 |
Tear Strength | 30.4 | kN/m | ASTM D624 |
Compression Set (70°C, 72 hr) | 27 | % | ASTM D395 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (-40°C) | No Break | ASTM D256 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
SCANAMID 6 B12^ F45 | Polykemi AB | Nylon 6 | SCANAMID 6 |
TEKNILID HS165 WP | Tekni-Films, a div of Tekni-Plex | Film, Coated Al Foil | TEKNILID |
VITAMIDE® AP36NT6567 | Jackdaw Polymers | Nylon 66 | VITAMIDE® |
Hifax TKC 243P C1V301 | LyondellBasell Industries | PP Copolymer | Hifax |
Sylvin 2900-75 Brown 7407 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |