| Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
| Manufacturer: | ResMart |
| Trademark: | ResMart Ultra |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | iPtQA4_ResMart-Ultra-TPU-80A-ES.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Polyester based TPU Shore 80A hardness for injection molding or extrusion applications |
| General Information | |
|---|---|
| Agency Ratings |
|
| RoHS Compliance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.18 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 80 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength | 29.6 | MPa | ASTM D638 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Elongation (Break) | 590 | % | ASTM D412 |
| Tear Strength | 85.0 | kN/m | ASTM D624 |
| Flammability | Nominal Value | Test Method | |
|---|---|---|---|
| Flame Rating | HB | UL 94 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature - Desiccant Dryer | 82.2 to 104 | °C | |
| Drying Time - Desiccant Dryer | 2.0 to 4.0 | hr | |
| Suggested Max Moisture | 0.010 | % | |
| Processing (Melt) Temp | 180 to 199 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Shuang-Bang WM-8157N | Shuang-Bang Industrial Corp. | Film, TPU | Shuang-Bang |
| Adiprene® LF 753D | Chemtura | PUR-Ether/TDI | Adiprene® |
| EPO-TEK® TV2001 | Epoxy Technology Inc. | Epoxy | EPO-TEK® |
| Optema™ TC 220 Molding | ExxonMobil Chemical | EMA | Optema™ |
| Sylvin 8200-80UV Red 6259 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |