Category: | SEBS , Styrene Ethylene Butylene Styrene Block Copolymer |
Manufacturer: | SO.F.TER. SPA |
Trademark: | Laprene® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | iOIRt8_Laprene-830000547.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Laprene® 830000547 is a Styrene Ethylene Butylene Styrene Block Copolymer (SEBS) material. It is available in Europe, Latin America, or North America for injection molding. Primary attribute of Laprene® 830000547: REACH Compliant. |
General Information | |
---|---|
Agency Ratings |
|
Appearance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.900 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A, 3 sec) | 34 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Set | 4 | % | ASTM D412 |
Tensile Stress 1(100% Strain) | 0.700 | MPa | ASTM D412 |
Tensile Strength 2 | 8.00 | MPa | ASTM D412 |
Tensile Elongation 3(Break) | 780 | % | ASTM D412 |
Tear Strength 4 | 26.0 | kN/m | ASTM D624 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 170 | °C | |
Middle Temperature | 180 | °C | |
Front Temperature | 180 | °C | |
Nozzle Temperature | 190 | °C | |
Mold Temperature | 20.0 to 40.0 | °C |
Note Message | |
---|---|
1 . | Die C |
2 . | Die C |
3 . | Die C |
4 . | Die C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
SILPURAN® 8630/60 | Wacker Chemie AG | Silicone | SILPURAN® |
Sylvin 8710-80 Black | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
ACCUTECH™ HP0334T10L1 | ACLO Compounders Inc. | PP Homopolymer | ACCUTECH™ |
CERTENE™ 705 SAN | Muehlstein | SAN | CERTENE™ |
LNP™ LUBRILOY™ K2000 compound | SABIC Innovative Plastics | Acetal (POM) Copolymer | LNP™ LUBRILOY™ |