Category: | TES , Styrenic Thermoplastic Elastomer |
Manufacturer: | Teknor Apex Company |
Trademark: | Telcar® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | hrAzmK_Telcar-TL-1934E.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Telcar®TL-1934E is a styrene thermoplastic elastomer (TES) material,. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is extrusion or injection molding. Telcar®The main characteristics of the TL-1934E are: flame retardant/rated flame. Telcar®The typical application fields of TL-1934E are: wire and cable |
General Information | |
---|---|
Uses |
|
Agency Ratings |
|
UL File Number |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.31 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (200°C/5.0 kg) | 18 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A) | 83 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength 1(Break, 23°C) | 10.7 | MPa | ASTM D412 |
Tensile Elongation 2(Break) | 630 | % | ASTM D412 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Strength in Air | ASTM D573 | ||
131°C, 3600 hr | -4.0 | % | ASTM D573 |
158°C, 168 hr | -11 | % | ASTM D573 |
Change in Ultimate Elongation in Air | ASTM D573 | ||
131°C, 3600 hr | -16 | % | ASTM D573 |
158°C, 168 hr | -15 | % | ASTM D573 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Continuous Use Temperature | 105 | °C | UL 1581 |
Brittleness Temperature | -59.0 | °C | ASTM D746 |
RTI Elec | 50.0 | °C | UL 746 |
RTI Imp | 50.0 | °C | UL 746 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Dielectric Strength | 35 | kV/mm | ASTM D149 |
Dielectric Constant | 2.40 | ASTM D150 | |
Dissipation Factor | 4.0E-3 | ASTM D150 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (1.35 to 1.55mm, All Colors) | V-0 | UL 94 | |
Oxygen Index | 26 | % | ASTM D2863 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 171 - 193 | °C | |
Middle Temperature | 177 - 199 | °C | |
Front Temperature | 182 - 204 | °C | |
Nozzle Temperature | 188 - 210 | °C | |
Processing (Melt) Temp | 188 - 210 | °C | |
Mold Temperature | 25.0 - 65.6 | °C | |
Injection Pressure | 1.38 - 6.89 | MPa | |
Injection Rate | Moderate-Fast | ||
Back Pressure | 0.172 - 0.345 | MPa | |
Screw Speed | 50 - 100 | rpm | |
Cushion | 3.81 - 25.4 | mm |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 166 - 188 | °C | |
Cylinder Zone 2 Temp. | 171 - 193 | °C | |
Cylinder Zone 3 Temp. | 177 - 199 | °C | |
Cylinder Zone 5 Temp. | 182 - 204 | °C | |
Die Temperature | 190 - 210 | °C |
Extrusion instructions |
---|
螺杆转速30 - 100 rpm |
Note Message | |
---|---|
1 . | 510 mm/min |
2 . | 510 mm/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
LNP™ THERMOCOMP™ DF002 compound | SABIC Innovative Plastics | PC | LNP™ THERMOCOMP™ |
LUVOCOM® 1301-7578 VP | Lehmann & Voss & Co. | PPS | LUVOCOM® |
OP - PC/ABS 604-I-FR | Oxford Polymers | PC+ABS | OP - PC/ABS |
Sylvin 6930X06 Orange 5117 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
Microthene® MP652962 | LyondellBasell Industries | HDPE | Microthene® |