30% GF, extremely chemically resistant and dimensionally stable PA6 type Characteristics:
Applications:
|
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Uses |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.36 | g/cm³ | ISO 1183 |
Water Absorption (Equilibrium, 23°C, 50% RH) | 2.1 | % | ISO 62 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 7500 | MPa | ISO 527-2/1/1 |
Tensile Stress (Yield) | 150 | MPa | ISO 527-2/50 |
Tensile Strain (Yield) | 3.0 | % | ISO 527-2/50 |
Flexural Modulus 1 | 7300 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength (23°C) | 10 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C) | 60 | kJ/m² | ISO 179/1eU |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature - Dry Air Dryer | 80.0 to 100 | °C | |
Drying Time - Dry Air Dryer | 2.0 to 4.0 | hr | |
Rear Temperature | 240 to 260 | °C | |
Middle Temperature | 250 to 270 | °C | |
Front Temperature | 250 to 280 | °C | |
Nozzle Temperature | 250 to 280 | °C | |
Processing (Melt) Temp | 260 to 290 | °C | |
Mold Temperature | 80.0 to 100 | °C |
Note Message | |
---|---|
1 . | 1.0 mm/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Sinvicomp SFR5800C2 | Teknor Apex Asia Pacific PTE. LTD. | PVC, Rigid | Sinvicomp |
apilon 52c® C 200 | API SpA | TPU-Polyester | apilon 52c® |
Flontech® FT-M02-1 | Guarniflon S.p.A. - Flontech Division | PTFE | Flontech® |
Generic ABS+PC - Unspecified | Generic | PC+ABS | Generic |
Polifor® E 16 TR/10 NATURALE | SO.F.TER. SPA | PP Copolymer | Polifor® |