Category: | NBR , Acrylonitrile Butadiene Rubber |
Manufacturer: | Nantex Industry Co., Ltd. |
Trademark: | NANCAR® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | gtSgLM_NANCAR-1203HD.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
NANCAR® 1203HD is a dry blend of 70 parts NANCAR NBR and 30 parts polyvinyl chloride. This polymer has sufficient stabilizer for normal aging conditions. It can be processed by normal mixing procedures. Its good processability for extrusion provides smooth surface on the resultant products. NANCAR® 1203HD has excellent resistance to abrasion, ozone, oils, fuels and solvents. It is suggested for use in cable jackets, belts, hose covers, shoe soles, rolls and sponge applications. |
General Information | |
---|---|
Additive |
|
Features |
|
Uses |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Mooney Viscosity (ML 1+4, 100°C) | 72 | MU | ASTM D1646 |
Acrylonitrile Content - Bound | 41.0 | % | Internal Method |
Elastomers | Nominal Value | Unit | |
---|---|---|---|
Compression Set - 70 hrs (100°C) | 52 | % |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Loss | 0.30 | % | ASTM D5688 |
Additional Information | Nominal Value | ||
---|---|---|---|
Ozone Resistance - 50 pphm X 40°C X 20% 1 | no crack |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A) | 78 |
Elastomers | Nominal Value | Unit | |
---|---|---|---|
Tensile Strength (Yield) | 12.9 | MPa | |
Tensile Elongation (Break) | 420 | % |
Aging | Nominal Value | Unit | |
---|---|---|---|
Change in Tensile Strength in Air (100°C, 70 hr) | 15 | % | |
Change in Ultimate Elongation in Air (100°C, 70 hr) | -33 | % | |
Change in Durometer Hardness in Air (100°C, 70 hr) | 3.0 | ||
Change in Tensile Strength | |||
100°C, 70 hr, in ASTM #1 Oil | 9.0 | % | |
100°C, 70 hr, in IRM 903 Oil | 6.0 | % | |
Change in Ultimate Elongation | |||
100°C, 70 hr, in ASTM #1 Oil | -38 | % | |
100°C, 70 hr, in IRM 903 Oil | -38 | % | |
Change in Durometer Hardness | |||
Shore A, 100°C, 70 hr, in ASTM #1 Oil | 12 | ||
Shore A, 100°C, 70 hr, in IRM 903 Oil | 8.0 | ||
Change in Volume | |||
100°C, 70 hr, in ASTM Oil #1 | -12 | % | |
100°C, 70 hr, in IRM 903 Oil | -6.0 | % |
Note Message | |
---|---|
1 . | at 24 hrs, 48 hrs, 72 hrs, 96 hrs, 168 hrs |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Rilsan® BMV0 P10 | Arkema | Nylon 11 | Rilsan® |
POLYVIN® PVC 6025D | A. Schulman Inc. | PVC, Unspecified | POLYVIN® |
NOVA PC 9050V | NOVA Polymers, Inc. | PC | NOVA PC |
EPO-TEK® 353ND-LH Premium | Epoxy Technology Inc. | Epoxy | EPO-TEK® |
Hydroxy-Purge 8C | InChem Corp. | TP, Unspecified | Hydroxy-Purge |