Category: | PP Homopolymer , Polypropylene Homopolymer |
Manufacturer: | ResMart |
Trademark: | ResMart Ultra |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | gfuZiA_ResMart-Ultra-HoPP-20-Adds.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Prime Homopolymer Polypropylene with nuc and antistat additives that provides a good balance of properties with good melt flow |
General Information | |
---|---|
Features |
|
Agency Ratings |
|
RoHS Compliance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.898 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 20 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Rockwell Hardness (R-Scale) | 112 | ASTM D785 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | 37.9 | MPa | ASTM D638 |
Tensile Elongation (Yield) | 7.5 | % | ASTM D638 |
Flexural Modulus | 1590 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (3.18 mm) | 27 | J/m | ASTM D256 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load (0.45 MPa, Unannealed) | 107 | °C | ASTM D648 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature - Desiccant Dryer | 79.4 | °C | |
Drying Time - Desiccant Dryer | 2.0 | hr | |
Processing (Melt) Temp | 191 to 232 | °C | |
Mold Temperature | 32.2 to 65.6 | °C | |
Injection Pressure | 68.9 to 103 | MPa |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Sipolprene® 58210 W | SIPOL S.p.A | TPC-ET | Sipolprene® |
EVERLON® TCE-30 | Ever Polymer Co., Ltd. | SEBS | EVERLON® |
DiaAlloy FE-504G | Mitsubishi Rayon America Inc. | PPE | DiaAlloy |
HiFill® PA6/6 GF14 IM HS L | Techmer Engineered Solutions | Nylon 66 | HiFill® |
ESTOPLAST XU 6340GY64 | Ester Industries Ltd. | Nylon 66 | ESTOPLAST XU |