| Category: | LLDPE , Linear Low Density Polyethylene |
| Manufacturer: | Lotte Chemical Corporation |
| Trademark: | SEETEC LLDPE |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | gfYM7g_SEETEC-LLDPE-UN324.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
UN324 is manufactured by Unipol process technology. UN324 has good mechanical properties and good processability. |
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Uses |
|
| RoHS Compliance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.920 | g/cm³ | ASTM D1505 |
| Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 1.1 | g/10 min | ASTM D1238 |
| Films | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Film Thickness - Tested | 40 | µm | |
| Tensile Strength | ASTM D882 | ||
| MD : Break, 40 µm, Blown Film | 43.1 | MPa | |
| TD : Break, 40 µm, Blown Film | 39.2 | MPa | |
| Tensile Elongation | ASTM D882 | ||
| MD : Break, 40 µm, Blown Film | 730 | % | |
| TD : Break, 40 µm, Blown Film | 750 | % | |
| Dart Drop Impact (40 µm, Blown Film) | 150 | g | ASTM D1709 |
| Elmendorf Tear Strength 1 | ASTM D1922 | ||
| MD : 40.0 µm | 49.0 | kN/m | |
| TD : 40.0 µm | 98.1 | kN/m |
| Optical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Gloss (45°, 40.0 µm, Blown Film) | 70 | ASTM D2457 | |
| Haze (40.0 µm, Blown Film) | 13 | % | ASTM D1003 |
| Note Message | |
|---|---|
| 1 . | Blown Film |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| QR Resin QR-1220LG(V) | QTR, Inc. | PC+ABS | QR Resin |
| Moplen EP300K | LyondellBasell Industries | PP Impact Copolymer | Moplen |
| Fainplast PVC RL 715/3 | Fainplast Compounds S.r.l | PVC, Rigid | Fainplast PVC |
| Ghaed SAN SAN-4 | Ghaed Basir Petrochemicals Co. | SAN | Ghaed SAN |
| Kepamid® 2325GFS | Korea Engineering Plastics Co., Ltd | Nylon 66 | Kepamid® |