| PEEK, 30 % glass fiber reinforced |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Resin ID (ISO 1043) |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.51 | g/cm³ | ISO 1183 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow | 0.90 | % | |
| Flow | 0.30 | % | |
| Water Absorption (Saturation, 23°C) | 0.020 | % | Internal Method |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 11800 | MPa | ISO 527-2 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength (23°C) | 7.5 | kJ/m² | ISO 179/1eA |
| Charpy Unnotched Impact Strength (23°C) | 60 | kJ/m² | ISO 179/1eU |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 328 | °C | ISO 75-2/A |
| Melting Temperature 1 | 343 | °C | ISO 11357-3 |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Volume Resistivity | 1.0E+16 | ohms·cm | IEC 60093 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flammability Classification (0.800 mm) | V-0 | IEC 60695-11-10, -20 |
| Note Message | |
|---|---|
| 1 . | 10°C/min |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Polyvel PLA HD-L01 PLA Impact Modifier (Opaque) | Polyvel Inc. | PLA | Polyvel PLA |
| Prime PE HMWPE 1000 SR | Primex Plastics Corporation | HMWPE | Prime PE |
| PRL ABS-GP1 | Polymer Resources Ltd. | ABS | PRL |
| Sinelec CCB7824 | Teknor Apex Asia Pacific PTE. LTD. | PP, Unspecified | Sinelec |
| Novalloy-S S66S4 | Daicel Polymer Ltd. | PC+ABS | Novalloy-S |