| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | Ravago Group |
| Trademark: | Ravamid® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | gWTQwq_Ravamid-R200-GF-10.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| 10% glass fibre reinforced PA6 compound for injection moulding |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.19 | g/cm³ | ISO 2781 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow | 1.1 | % | |
| Flow | 0.30 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 5200 | MPa | ISO 527-2 |
| Tensile Stress (Yield) | 100 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 3.5 | % | ISO 527-2 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength | 6.0 | kJ/m² | ISO 180/1A |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature | |||
| 0.45 MPa, Unannealed | 210 | °C | ISO 75-2/B |
| 1.8 MPa, Unannealed | 195 | °C | ISO 75-2/A |
| Vicat Softening Temperature | 206 | °C | ISO 306/A120 |
| Melting Temperature | 220 to 225 | °C |
| Flammability | Nominal Value | Test Method | |
|---|---|---|---|
| Flame Rating 1(1.60 mm) | HB | Internal Method |
| Note Message | |
|---|---|
| 1 . | UL94 internally tested |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Premier HD11051 | Premier Polymers, LLC. | HDPE | Premier |
| Sinvicomp SIM6039 | Teknor Apex Asia Pacific PTE. LTD. | PVC, Flexible | Sinvicomp |
| LAMIGAMID® 100 | Schwartz Technical Plastic | Nylon 6 | LAMIGAMID® |
| Karina BROWN PVC COMPOUND 800-36/61-ERYB | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |