Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
Manufacturer: | Shanghai Utomer Material Science Co., Ltd. |
Trademark: | Utomer |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | gKfnNu_Utomer-UT380.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Utomer TPU which include ester and ether type. It's suitable for calendering and extrusion, which are used for shoes and clothing leatherette and compounding with PVC. |
General Information | |
---|---|
Uses |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.20 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A) | 78 to 82 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Abrasion Loss | 45.0 | mm³ | DIN 53516 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ASTM D412 | ||
100% Strain | 10.0 | MPa | |
300% Strain | 14.0 | MPa | |
Tensile Strength | 30.0 | MPa | ASTM D412 |
Tensile Elongation (Break) | 600 | % | ASTM D412 |
Tear Strength | 0.100 | kN/m | ASTM D624 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Glass Transition Temperature | -15.0 | °C | ASTM D3418 |
Melting Temperature | 185 to 200 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
ColorRx® PP1-2000RX | LTL Color Compounders, Inc. | PP Homopolymer | ColorRx® |
Grilamid® LV-30H FWA nat | EMS-GRIVORY | Nylon 12 | Grilamid® |
Petrothene® NA340185 | LyondellBasell Industries | LDPE | Petrothene® |
Vaycron® VA2030 | INEOS Compounds | TPE | Vaycron® |
NORYL GTX™ GTX902D resin | SABIC Innovative Plastics Europe | PPE+PS+Nylon | NORYL GTX™ |