| Category: | PP Homopolymer , Polypropylene Homopolymer |
| Manufacturer: | SIBUR, LLC |
| Trademark: | TOLEN |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | gKOAUQ_TOLEN-H233-FF.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| PP H233 FF is a polypropylene homopolymer with narrow molecular mass distribution. The product features high fluidity, an optimal stabilizing package, balanced physical and mechanical properties, and resistance to discoloration of final products in outdoor conditions. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 23 | g/10 min | Internal Method |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress 1(Yield) | 30.0 | MPa | Internal Method |
| Tensile Strain 2(Yield) | 11 | % | Internal Method |
| Flexural Modulus 3 | 1400 | MPa | Internal Method |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength (23°C) | 2.0 | kJ/m² | Internal Method |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (0.45 MPa, Unannealed) | 80.0 | °C | Internal Method |
| Vicat Softening Temperature | 156 | °C | Internal Method 4 |
| Note Message | |
|---|---|
| 1 . | 50 mm/min |
| 2 . | 50 mm/min |
| 3 . | 5.0 mm/min |
| 4 . | A (10N) |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| ZYLAR® 550 | INEOS Styrolution Group GmbH | MMBS | ZYLAR® |
| CALIBRE™ 203-22 | Trinseo | PC | CALIBRE™ |
| DOMAMID® 6B30 | DOMO Engineering Plastics SPA | Nylon 6 | DOMAMID® |
| SCHULAMID® 66 GF 33 FC | A. Schulman Europe | Nylon 66 | SCHULAMID® |
| Monprene® RG-17280 (PRELIMINARY DATA) | Teknor Apex Company | TPE | Monprene® |