| Category: | SBR, Emulsion , Emulsion Styrene Butadiene Rubber |
| Manufacturer: | INSA |
| Trademark: | Emulprene® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | g7k9NE_Emulprene-1013A.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Description: E1013A is a styrene-butadiene copolymer, hot polymerized using a fatty acid soap. Previously to the alum-acid coagulation, a non-staining stabilizer is added in the manufacturing process. Applications: E1013A is suitable for adhesive applications it is particularly used for can-sealing compounds, tire liners, mechanical goods, including auto mounts, and household products. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Mooney Viscosity | ASTM D1646 | ||
| ML 1+4, 100°C 1 | 55 to 65 | MU | |
| ML 1+4, 100°C | 40 to 50 | MU | |
| Ash Content | < 1.0 | % | ASTM D5667 |
| Organic Acid | 3.5 to 5.5 | % | ASTM D5774 |
| Soap | < 0.30 | % | ASTM D5774 |
| Styrene Content - Bound | 42 to 45 | % | ASTM D5775 |
| Volatile Matter | < 1.0 | % | ASTM D5668 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 14.0 to 16.0 | MPa | ASTM D3185 |
| Tensile Strength | 20.0 to 24.0 | MPa | ASTM D3185 |
| Tensile Elongation (Break) | 300 to 500 | % | ASTM D3185 |
| Note Message | |
|---|---|
| 1 . | Compound |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Fainplast PVC GS 6612 | Fainplast Compounds S.r.l | PVC, Unspecified | Fainplast PVC |
| K-vinyl 125 Deg C Rating Insulation (Auto) | Technovinyl Polymers India Ltd. | PVC, Unspecified | K-vinyl |
| OmniLon™ PA6/6 MF40 | OMNI Plastics, LLC | Nylon 66 | OmniLon™ |
| Plaslube® PC / PBT IM 5230 | Techmer Engineered Solutions | PC+PBT | Plaslube® |
| Crastin® T843FR NC010 | DuPont Performance Polymers | PBT | Crastin® |