DSM's Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS-like properties and good temperature resistance. It produces colorless, functional, accurate parts that simulate an acrylic appearance. Based on the Oxetane Advantage™, the parts also have improved water- resistance over the original Somos® WaterClear 10120 resin. Somos® WaterClear Ultra is a fast, low viscosity, general-purpose resin. Applications This high-temperature resistant, ABS-like photopolymer is used in solid imaging processes, like stereolithography, to build three-dimensional parts. Somos® WaterClear Ultra is ideal for applications requiring optical clarity, such as automotive lenses, bottles, fluid flow analysis, packaging prototypes, light pipes and more. Somos® WaterClear Ultra can also be used for concept, functional models and master patterns. |
General Information | |
---|---|
Features |
|
Uses |
|
Appearance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.13 | g/cm³ | |
Water Absorption (Equilibrium) | 1.1 | % | ASTM D570 |
Viscosity (30°C) | 165 | mPa·s |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Poisson's Ratio | 0.40 to 0.42 | ASTM D638 |
Additional Information | Nominal Value | Unit | |
---|---|---|---|
Critical Exposure | 10.0 | mJ/cm² | |
Penetration Depth | 165.1 | µm |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore D) | 86 to 87 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 2860 to 2900 | MPa | ASTM D638 |
Tensile Strength (Break) | 55.0 to 56.0 | MPa | ASTM D638 |
Tensile Elongation | ASTM D638 | ||
Yield | 4.0 | % | |
Break | 6.0 to 9.0 | % | |
Flexural Modulus | 2410 to 2570 | MPa | ASTM D790 |
Flexural Strength | 82.0 to 85.0 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact | 23 to 26 | J/m | ASTM D256A |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load | ASTM D648 | ||
0.45 MPa, Unannealed 1 | 59.0 to 61.0 | °C | |
0.45 MPa, Unannealed | 46.0 to 47.0 | °C | |
1.8 MPa, Unannealed 2 | 49.0 to 50.0 | °C | |
1.8 MPa, Unannealed | 42.0 to 43.0 | °C | |
Glass Transition Temperature | 42.0 to 46.0 | °C | ASTM E1545 |
CLTE - Flow | ASTM E831 | ||
-40 to 0°C | 6.4E-5 to 6.7E-5 | cm/cm/°C | |
0 to 50°C | 8.8E-5 to 9.3E-5 | cm/cm/°C | |
50 to 100°C | 1.6E-4 to 1.7E-4 | cm/cm/°C | |
100 to 150°C | 1.5E-4 to 1.7E-4 | cm/cm/°C |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Dielectric Strength | 15 to 16 | kV/mm | ASTM D149 |
Dielectric Constant | ASTM D150 | ||
60 Hz | 3.00 to 3.20 | ||
1 kHz | 3.30 to 3.60 | ||
1 MHz | 3.00 to 3.20 |
Optical | Nominal Value | Test Method | |
---|---|---|---|
Refractive Index | 1.520 | ASTM D542 |
Note Message | |
---|---|
1 . | with Thermal Postcure |
2 . | with Thermal Postcure |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
ACCUCOMP™ CP0403L | ACLO Compounders Inc. | PP Copolymer | ACCUCOMP™ |
NYLEM® 66 GFR 25 | EMAS Plastik San.Tic.AS. | Nylon 66 | NYLEM® |
Borcoat™ ME0433 | Borealis AG | PE, Unspecified | Borcoat™ |
Grilamid® L 25 nat | EMS-GRIVORY | Nylon 12 | Grilamid® |
ESTOPLAST EP 4000NN01 | Ester Industries Ltd. | PBT | ESTOPLAST EP |