Category: | PP Random Copolymer , Polypropylene Random Copolymer |
Manufacturer: | Borealis AG |
Trademark: | Borealis PP |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | fOmEmd_Borealis-PP-RB206MO-06.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
RB206MO-06 is a random copolymer with good transparency and contact clarity, very good gloss and surface finish The high stiffness of this grade allows for a reduction in cycle time. This grade also features high heat distortion temperature. The additives are optimized to provide reduced tendency for mould plate-out. |
General Information | |
---|---|
Features |
|
Uses |
|
Appearance |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.902 | g/cm³ | ISO 1183 |
Apparent Density | 0.50 to 0.60 | g/cm³ | |
Melt Mass-Flow Rate (MFR) (230°C/1.9 kg) | 1.9 | g/10 min | ISO 1133 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 1150 | MPa | ISO 527-2 |
Tensile Stress (Yield) | 26.0 | MPa | ISO 527-2/50 |
Tensile Strain (Yield) | 12 | % | ISO 527-2/50 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength (23°C) | 7.0 | kJ/m² | ISO 179/1eA |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (0.45 MPa, Unannealed) | 86.0 | °C | ISO 75-2/B |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 190 to 220 | °C | |
Melt Temperature | 180 to 220 | °C | |
Die Temperature | 180 to 220 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
POPTREE 6001 | POLYROCKS CHEMICAL CO., LTD | PE, Unspecified | POPTREE |
RTP EMI 660.7 FR | RTP Company | ABS | RTP |
Carbotex K-20UVR28 | Kotec Corporation | PC | Carbotex |
Lucky Enpla LGF6300 | Lucky Enpla Co LTD | PP, Unspecified | Lucky Enpla |
Plexiglas® LED 8N LD24 | Evonik Industries AG | Acrylic (PMMA) | Plexiglas® |