| Category: | Acetal (POM) Copolymer , Acetal (POM) Copolymer |
| Manufacturer: | Korea Engineering Plastics Co., Ltd |
| Trademark: | Kepital® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | e5r4nB_KepitalMF3025.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Milled fiber 25% filled and partially reinforced grade. MF3025 is suitable for parts requiring low warpage than those of the FG series which is longer glass fiber |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.59 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) | 16 | g/10 min | ISO 1133 |
| Molding Shrinkage - Flow (3.00 mm) | 1.3 | % | ISO 294-4 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Break, 23°C) | 78.0 | MPa | ISO 527-2 |
| Nominal Tensile Strain at Break (23°C) | 4.9 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 5530 | MPa | ISO 178 |
| Flexural Stress (23°C) | 129 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | 3.8 | kJ/m² | ISO 179/1eA |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Surface Resistivity | 1.0E+16 | ohms | IEC 60093 |
| Volume Resistivity | 1.0E+14 | ohms·cm | IEC 60093 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating | HB | UL 94 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| TEDUR® L FC 9510-5 | ALBIS PLASTIC GmbH | PPS | TEDUR® |
| Telcar® TL-1268A | Teknor Apex Company | TPE | Telcar® |
| Vyncolit® G865 | Vyncolit N.V. | Phenolic | Vyncolit® |
| Westlake PVDF Film | Westlake Plastics Company | PVDF | Westlake |
| Elastron® G G100.A50.N | Elastron USA, Inc. | SEBS | Elastron® G |