Category: | TPE , Thermoplastic Elastomer |
Manufacturer: | Mitsubishi Chemical Performance Polymers, Inc. |
Trademark: | tefabloc® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | dgUBFk_tefabloc-TP-SD-310-80A.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
tefabloc®TP SD 310 80A is a thermoplastic elastomer (TPE) material,. This product is available in North America or Europe. The processing method is injection molding. tefabloc®The main features of TP SD 310 80A are:
Typical application areas include:
|
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Resin ID (ISO 1043) |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.04 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 28 | g/10 min | ISO 1133 |
Molding Shrinkage | Internal method | ||
Vertical flow direction | 1.2 | % | Internal method |
Flow direction | 0.90 | % | Internal method |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A, 15 sec, Injection Molded) | 80 | ISO 868 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Abrasion | 160 | mm³ | DIN 53516 |
Aging | Nominal Value | Unit | |
---|---|---|---|
Resistance to Aging | 125 | °C |
Thermal | Nominal Value | Unit | |
---|---|---|---|
Service Temperature | -50 - 70 | °C |
Additional Information | Nominal Value | Test Method | |
---|---|---|---|
Color Fastness 1 | 4/5 | ISO 105-A02 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ISO 37 | ||
20% strain | 3.40 | MPa | ISO 37 |
100% strain | 4.40 | MPa | ISO 37 |
Tensile Stress (Break) | 7.20 | MPa | ISO 37 |
Tensile Elongation (Break) | 600 | % | ISO 37 |
Tear Strength 2 | 42 | kN/m | ISO 34-1 |
Compression Set 3 | ISO 815 | ||
23°C, 22 hr | 37 | % | ISO 815 |
50°C, 22 hr 4 | 40 | % | ISO 815 |
50°C, 22 hr 5 | 56 | % | ISO 815 |
70°C, 22 hr 6 | 46 | % | ISO 815 |
70°C, 22 hr 7 | 67 | % | ISO 815 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 160 | °C | |
Middle Temperature | 170 | °C | |
Front Temperature | 180 | °C | |
Injection Rate | Moderate | ||
Screw Compression Ratio | 2.5:1.0 - 3.0:1.0 |
Injection instructions |
---|
Screw Speed: Medium |
Note Message | |
---|---|
1 . | 1000 hr |
2 . | Method B, right-angle specimen (without cut) |
3 . | Type B |
4 . | relaxation 50°C |
5 . | relaxation 23°C |
6 . | relaxation 70°C |
7 . | relaxation 23°C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Vi-Chem PVC PNC87-5 | Vi-Chem Corporation | PVC, Unspecified | Vi-Chem PVC |
Toraycon® 1101G-X08 | Toray Resin Company | PBT | Toraycon® |
Aegis® H85NP | Honeywell | Nylon 6 | Aegis® |
Bynel® 3126 | DuPont Packaging & Industrial Polymers | EVA | Bynel® |
OnFlex™ S FR 40A-3S1841 | PolyOne Corporation | TPE | OnFlex™ |