Category: | SEBS , Styrene Ethylene Butylene Styrene Block Copolymer |
Manufacturer: | Franplast S.r.l. |
Trademark: | Chemiton |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | dgAZWl_Chemiton-GTB5FA-80E.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
SBS/SEBS compounds, with or without foaming agent, food contact approved. Injection molding and extrusion grades available. Properties and performances similar corks. Application:
|
General Information | |
---|---|
Features |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 30 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Shore Hardness (Shore A) | 80 | ISO 868 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Break) | 4.50 | MPa | ISO 527-2 |
Nominal Tensile Strain at Break | 700 | % | ISO 527-2 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tear Strength | 30 | kN/m | ISO 34-1 |
Thermal | Nominal Value | Unit | |
---|---|---|---|
Service Temperature | -30 to 90 | °C |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Time | 0.0 | hr | |
Rear Temperature | 155 to 175 | °C | |
Middle Temperature | 170 to 190 | °C | |
Front Temperature | 175 to 195 | °C | |
Nozzle Temperature | 175 to 195 | °C | |
Mold Temperature | 30.0 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 205 A TFE 13 SI 2 | RTP Company | Nylon 6 | RTP |
WanBlend® WHT-HF8675 | Wanhua Chemical Group Co., Ltd. | TPU-Polyether | WanBlend® |
UNITAL® LZU | Nytef Plastics, Ltd. | Acetal (POM) Copolymer | UNITAL® |
NORYL™ WCP921 resin | SABIC Innovative Plastics Asia Pacific | PPE+TPE | NORYL™ |
INSULCAST® RTVS 27 | ITW Polymers Coatings North America | Silicone Rubber, RTV-2 | INSULCAST® RTVS |