Elastron® V V250.A58.B

Category: TPV , Thermoplastic Vulcanizate
Manufacturer: Elastron USA, Inc.
Trademark: Elastron® V
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: dX3kwF_Elastron-V-V250-A58-B.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
A soft, black TPV (EPDM /PP ) material belongs to thermoplastic elastomer (TPE) family with superior UV resistance and excellent compression set. This product is specially designed for weatherseal applications.

Bondable to: PP, EVA, PE
General Information
Features
  • Bondability
  • Good UV Resistance
  • Soft
Uses
  • Seals
RoHS Compliance
  • RoHS Compliant
Appearance
  • Black
Forms
  • Pellets
Processing Method
  • Injection Molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 0.970g/cm³ASTM D792
Molding Shrinkage ASTM D955
    Flow 2.6%
    Across Flow 1.4%
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore A)58ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Stress ASTM D412
    100% Strain 1.70MPa
    300% Strain 2.80MPa
Tensile Strength (Break)5.00MPaASTM D412
Tensile Elongation (Break)650%ASTM D412
Tear Strength 24.0kN/mASTM D624
Compression Set ASTM D395
    23°C, 22 hr 16%
    70°C, 22 hr 34%
    100°C, 22 hr 51%
Additional InformationNominal ValueTest Method
Ozone Resistance - Stressed No CracksASTM D518
InjectionNominal ValueUnit
Drying Temperature 90.0°C
Drying Time 2.0hr
Suggested Max Regrind 20%
Rear Temperature 155 to 175°C
Middle Temperature 165 to 185°C
Front Temperature 170 to 190°C
Nozzle Temperature 180 to 210°C
Mold Temperature 25.0 to 50.0°C
Resin Grade Manufacturer Category Trademark
Moplen EP640V LyondellBasell Industries PP Impact Copolymer Moplen
BESTNYL SE25VI02A Triesa Plastics Nylon 66 BESTNYL
Petrothene® YR92126 LyondellBasell Industries XLPE Petrothene®
Sumiliteresin® PR-F-151B SBHPP Phenolic Sumiliteresin®
Sylvin 9302-70 Brown 7380 Sylvin Technologies Incorporated PVC, Unspecified Sylvin