| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | Wellman Engineering Resins |
| Trademark: | Wellamid® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | dLAs5u_Wellamid-T-731E-BK.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Wellamid® T-731E-BK is a Polyamide 6 (Nylon 6) material filled with 10% filler. It is available in Asia Pacific, Europe, Latin America, or North America. Primary attribute of Wellamid® T-731E-BK: Wear Resistant. |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.18 | g/cm³ | ISO 1183 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow | 1.3 to 1.7 | % | |
| Flow | 1.6 to 2.0 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Yield, 23°C) | 65.0 | MPa | ISO 527-2 |
| Tensile Strain (Break, 23°C) | 30 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 2600 | MPa | ISO 178 |
| Flexural Stress (23°C) | 90.0 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength (23°C) | 8.0 | kJ/m² | ISO 180 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 60.0 | °C | ISO 75-2/A |
| Melting Temperature (DSC) | 220 | °C | ISO 3146 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Silopren® LSR 3376/50 | Momentive Performance Materials Inc. | Silicone Rubber, LSR | Silopren® |
| VESTOLIT® E 6007 | VESTOLIT GmbH & Co. KG | PVC, Unspecified | VESTOLIT® |
| Akulon® K224-G3 | DSM Engineering Plastics | Nylon 6 | Akulon® |
| ARCEL® 640 (5.00 pcf) | NOVA Chemicals | PS+PE | ARCEL® |
| Axiall PVC 19463 | Axiall Corporation | PVC, Flexible | Axiall PVC |