Category: | PP, Unspecified , Polypropylene |
Manufacturer: | Polykemi AB |
Trademark: | POLYfill |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | dC6tIp_POLYfill-PP-CIQ10015ER-UV.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Mineral reinforced |
General Information | |
---|---|
Filler / Reinforcement |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.990 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 14 | g/10 min | ISO 1133 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow | 1.3 to 1.6 | % | |
Flow | 1.3 to 1.6 | % |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore D, 15 sec) | 56 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | 20.0 | MPa | ISO 527-2 |
Tensile Strain (Break) | 110 | % | ISO 527-2 |
Flexural Modulus (23°C) | 1400 | MPa | ISO 178 |
Flexural Stress | 35.0 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | ||
-20°C | 4.0 | kJ/m² | |
23°C | 12 | kJ/m² |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature 1 | |||
0.45 MPa, Unannealed | 87.0 | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 47.0 | °C | ISO 75-2/A |
Vicat Softening Temperature | |||
-- | 142 | °C | ISO 306/A50 |
-- | 63.0 | °C | ISO 306/B50 |
Note Message | |
---|---|
1 . | 120°C/hr |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Tempalux® Film | Westlake Plastics Company | PEI | Tempalux® |
TEREZ PA 6 7500 GF 30 FL HF/1 | TER HELL PLASTIC GMBH | Nylon 6 | TEREZ PA 6 |
Buna® EP T 5459 CL | LANXESS Corporation | EPDM | Buna® EP |
Hifax PPU 1752S2S003 | LyondellBasell Industries | PP Copolymer | Hifax |
Hapweld™ 39 | Hapco Inc. | TP, Unspecified | Hapweld™ |