General Information | |
---|---|
Features |
|
Uses |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density (23°C) | 1.12 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (220°C/10.0 kg) | 16 | g/10 min | ISO 1133 |
Melt Volume-Flow Rate (MVR) (220°C/10.0 kg) | 16.7 | cm³/10min | ISO 1133 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Rockwell Hardness (R-Scale, 2.50 mm) | 122 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Yield) | 77.0 | MPa | ISO 527-2/5 |
Flexural Modulus 1 | 3600 | MPa | ISO 178 |
Flexural Stress 2 | 122 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength (23°C) | 1.3 | kJ/m² | ISO 179 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 79.3 | °C | ISO 75-2/A |
Vicat Softening Temperature | 97.9 | °C | ISO 306/B |
Note Message | |
---|---|
1 . | 2.0 mm/min |
2 . | 2.0 mm/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 107 CC HB | RTP Company | PP, Unspecified | RTP |
DOMAMID® 66V0M | DOMO Engineering Plastics SPA | Nylon 66 | DOMAMID® |
Petra® 130 FR BK-112 | BASF Corporation | PET | Petra® |
TOTAL Polypropylene Aceso® PPM H250 S01 | TOTAL Refining & Chemicals | PP Homopolymer | TOTAL Polypropylene |
Sylvin 6920X08 Brown 7408 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |