Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
Manufacturer: | Wanhua Chemical Group Co., Ltd. |
Trademark: | Wanthane® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | ctc8kW_WanthaneWHT56170.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
TYPE: Polyester-based grade Extrusion grade FEATURES: Good low temperature flexibility, wide process window, excellent partner for PVC Applications: Hose jackets, films, etc. |
General Information | |
---|---|
Features |
|
Uses |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.19 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A) | 70 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ASTM D412 | ||
100% strain | 2.50 | MPa | ASTM D412 |
300% strain | 4.00 | MPa | ASTM D412 |
Tensile Strength (Break) | 20.0 | MPa | ASTM D412 |
Tensile Elongation (Break) | 800 | % | ASTM D412 |
Tear Strength | 55.0 | kN/m | ASTM D624 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 90 - 100 | °C | |
Drying Time | 2.0 - 3.0 | hr | |
Suggested Max Moisture | 0.030 | % | |
Cylinder Zone 1 Temp. | 150 | °C | |
Cylinder Zone 2 Temp. | 155 | °C | |
Cylinder Zone 3 Temp. | 160 | °C | |
Cylinder Zone 4 Temp. | 165 | °C | |
Adapter Temperature | 170 | °C | |
Die Temperature | 160 - 165 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
VALOX™ VC120 resin | SABIC Innovative Plastics Asia Pacific | PBT | VALOX™ |
ADDINYL A2H M30 | ADDIPLAST | Nylon 66 | ADDINYL |
Hanwha Total PP BI492 | HANWHA TOTAL PETROCHEMICALS Co., Ltd. | PP, Unspecified | Hanwha Total PP |
HiFill FR® ABS FR AS | Techmer Engineered Solutions | ABS | HiFill FR® |
LG PMMA IF870S | LG MMA Corp. | Acrylic (PMMA) | LG PMMA |