Mirakutoran® TPU E574

Category: TPU Alloy , Thermoplastic Polyurethane Elastomer Alloy
Manufacturer: Japan Mirakutoran Inc.
Trademark: Mirakutoran® TPU
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: ciuptN_Mirakutoran-TPU-E574.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Our TPU "Mirakutoran ®" has the following outstanding features.
  • Has excellent wear resistance
  • Tensile strength, high mechanical strength and tear strength
  • Is a wide range of hardness
  • High impact strength
  • Oil resistance and good chemical resistance
  • Excellent low temperature properties, weather resistance, ozone resistance and is also good
  • Flexible rubber elastic, vibration-effective silencing

Compared to other urethane elastomer thermoplastic that is more
  • Playback can be processed
  • Vulcanization process without curing reaction, very high productivity
  • Resins and other polymer is easy
  • Solution is easily dissolved in solvent process

Mirakutoran to the standard type E and P are two types.

Type E has a certain cross-linked structure in the molecule, and excellent mechanical strength and compression set. P type is characterized by good liquidity linear structure

General Information
Features
  • Shock absorption
  • Impact resistance, good
  • Good strength
  • Good flexibility
  • Good tear strength
  • Ozone resistance
  • Low temperature resistance
  • Good chemical resistance
  • Good wear resistance
  • Good weather resistance
  • Oil resistance
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.23g/cm³ASTM D792
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore D, 23°C, 2.00mm, injection molding)72 - 76ASTM D2240
MechanicalNominal ValueUnitTest Method
Taber Abrasion Resistance (23°C, 1000 Cycles, 1000 g, H-22 Wheel)90.0mgASTM D1044
ElastomersNominal ValueUnitTest Method
Tensile Stress 1(100% strain, 23°C, 2.00mm)42.0MPaASTM D412
Tensile Strength 2(Yield, 23°C, 2.00 mm)56.0MPaASTM D412
Tensile Elongation 3(Break, 23°C, 2.00 mm)350%ASTM D412
Tear Strength 4(23°C, 2.00 mm)294kN/mASTM D624
Compression Set (70°C, 22 hr)42%ASTM D395
Rebound Resilience (23°C, 2.00 mm)39%
ThermalNominal ValueUnitTest Method
Vicat Softening Temperature 151°CASTM D1525 5
Additional Information
Test Methods: JIS K7311, K6262, K7206
Note Message
1 .300 mm/min
2 .300 mm/min
3 .300 mm/min
4 .300 mm/min
5 .压 力1 (10N)
Resin Grade Manufacturer Category Trademark
TECHNYL STAR™ AFX 218 V50 BLACK 31N Solvay Engineering Plastics Nylon 66 TECHNYL STAR™
SINOF DH-F22M SINOF HI-TECH MATERIAL CO. LTD PVDF SINOF
Axiall PVC 4590 Axiall Corporation PVC, Flexible Axiall PVC
Hanwha Total PP TB72W HANWHA TOTAL PETROCHEMICALS Co., Ltd. PP, High Crystal Hanwha Total PP
EPAMOULD 272D12 Epaflex Polyurethanes S.R.L. TPU-Polyester EPAMOULD