Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | DOMO Engineering Plastics GmbH |
Trademark: | DOMAMID® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | cdZs4S_DOMAMID-A1-501-I1-N.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Polyamide 6, impact modified, natural |
General Information | |
---|---|
Additive |
|
Features |
|
Appearance |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.10 | g/cm³ | ISO 1183 |
Melt Volume-Flow Rate (MVR) (275°C/5.0 kg) | 165 | cm³/10min | ISO 1133 |
Molding Shrinkage 1 | ISO 294-4 | ||
Across Flow : 23°C, 72 hr | 1.5 | % | |
Flow : 23°C, 72 hr | 1.7 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 2700 | MPa | ISO 527-2/1A/1 |
Tensile Stress | ISO 527-2/1A/5 | ||
Yield | 65.0 | MPa | |
Break | 50.0 | MPa | |
Tensile Strain (Break) | > 20 | % | ISO 527-2/1A/20 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength (23°C) | 12 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C) | No Break | ISO 179/1eU |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Melting Temperature | 221 | °C | ISO 11357-3 |
Note Message | |
---|---|
1 . | 50%RH, between 16 to 72 hrs |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Sarlink® TPE ME-2385N | Teknor Apex Company | TPE | Sarlink® TPE |
NILENE® E12 | Taro Plast S.p.A. | PP Copolymer | NILENE® |
Bergadur™ BR3300-8024 RS NC018 | PolyOne Corporation | PBT | Bergadur™ |
Fainplast PVC FKA 0753 | Fainplast Compounds S.r.l | PVC, Unspecified | Fainplast PVC |
Hytrel® G4074 | DuPont Performance Polymers | TPC-ET | Hytrel® |