RTP 132 HI

Category: PP, Unspecified , Polypropylene
Manufacturer: RTP Company
Trademark: RTP
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: cacCSU_RTP-132-HI.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
High Impact - Talc
General Information
Filler / Reinforcement
  • Talc, 30% Filler by Weight
Features
  • High Impact Resistance
RoHS Compliance
  • Contact Manufacturer
Processing Method
  • Injection Molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.12g/cm³ASTM D792
Molding Shrinkage - Flow (3.20 mm)0.70 to 1.1%ASTM D955
MechanicalNominal ValueUnitTest Method
Tensile Modulus 3100MPaASTM D638
Tensile Strength 20.7MPaASTM D638
Tensile Elongation (Yield)> 10%ASTM D638
Flexural Modulus 2070MPaASTM D790
Flexural Strength 33.8MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (3.20 mm)200J/mASTM D256
Unnotched Izod Impact (3.20 mm)1300J/mASTM D4812
ThermalNominal ValueUnitTest Method
Deflection Temperature Under Load (1.8 MPa, Unannealed)71.1°CASTM D648
FlammabilityNominal ValueTest Method
Flame Rating (1.50 mm, ** Values per RTP Company testing.)HBUL 94
Additional InformationNominal ValueUnit
Primary Additive 30%
InjectionNominal ValueUnit
Drying Temperature 79.4°C
Drying Time 2.0hr
Processing (Melt) Temp 191 to 232°C
Mold Temperature 32.2 to 65.6°C
Injection Pressure 68.9 to 103MPa
Resin Grade Manufacturer Category Trademark
DOMAMID® 6AF IE DOMO Engineering Plastics SPA Nylon 6 DOMAMID®
Multilon® TN-7504 TEIJIN LIMITED PC+ABS Multilon®
Sylvin 4225-75 White 1498 Sylvin Technologies Incorporated PVC, Unspecified Sylvin
Sylvin 8980-80 Black Sylvin Technologies Incorporated PVC, Unspecified Sylvin
PENTAMID B GV35 H black PENTAC Polymer GmbH Nylon 6 PENTAMID B