| Category: | PP+EPDM , Polypropylene + EPDM Rubber |
| Manufacturer: | Polykemi AB |
| Trademark: | POLYelast |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | c2FVOV_POLYelast-TPE-EC88R.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| PP/EPDM |
| General Information |
|---|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.900 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 3.0 | g/10 min | ISO 1133 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow | 0.90 to 1.1 | % | |
| Flow | 0.90 to 1.1 | % |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness | ASTM D2240 | ||
| Shore A, 15 sec | 88 | ||
| Shore D, 15 sec | 30 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | 15.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | > 55 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 450 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179 | ||
| -20°C | No Break | ||
| 23°C | No Break |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature 1(0.45 MPa, Unannealed) | 56.0 | °C | ISO 75-2/B |
| Note Message | |
|---|---|
| 1 . | 120°C/hr |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 1401 B L | RTP Company | PESU | RTP |
| Ultralloy™ 206 | Hapco Inc. | TP, Unspecified | Ultralloy™ |
| NOPLA® KE901 | Kolon Plastics, Inc. | PEN | NOPLA® |
| Hostaform® C 13031 K | Celanese Corporation | Acetal (POM) Copolymer | Hostaform® |
| Karina COMP. PVC NATURAL -E 600-DA-35/ 1-A-IS | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |