Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | Solvay Engineering Plastics |
Trademark: | TECHNYL® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | baihGo_TECHNYLC246SINATURAL.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
TECHNYL® C 246SI Natural is an unfilled polyamide 6, with improved impact resistance, for injection moulding. This grade offers high impact strength, flexibility and good surface aspect. |
General Information | |
---|---|
Additive |
|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Resin ID (ISO 1043) |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.06 | -- | g/cm³ | ISO 1183/A |
Water Absorption (23°C, 24 hr) | 1.0 | -- | % | ISO 62 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus (23°C) | 1900 | 700 | MPa | ISO 527-2/1A |
Tensile Stress | ISO 527-2/1A | |||
Yield, 23°C | 45.0 | 36.0 | MPa | ISO 527-2/1A |
Fracture, 23°C | 46.0 | 36.0 | MPa | ISO 527-2/1A |
Tensile Strain | ISO 527-2 | |||
Yield, 23°C | 4.0 | -- | % | ISO 527-2 |
Fracture, 23°C | 120 | -- | % | ISO 527-2 |
Flexural Modulus (23°C) | 1700 | 500 | MPa | ISO 178 |
Flexural Stress (23°C) | 64.0 | 21.0 | MPa | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | |||
-30°C | 23 | -- | kJ/m² | ISO 179/1eA |
23°C | 110 kJ/m² | No Break | ISO 179/1eA | |
Charpy Unnotched Impact Strength (23°C) | No Break | -- | ISO 179/1eU | |
Notched Izod Impact (23°C) | 110 | -- | kJ/m² | ISO 180 |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 51.0 | -- | °C | ISO 75-2/Af |
Melting Temperature | 220 | -- | °C | ISO 11357-3 |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 80 | °C | |
Suggested Max Moisture | 0.20 | % | |
Rear Temperature | 240 - 260 | °C | |
Middle Temperature | 250 - 270 | °C | |
Front Temperature | 260 - 280 | °C | |
Mold Temperature | 70 - 90 | °C |
Injection instructions |
---|
The material is supplied in airtight bags, ready for use. In case that the virgin material has absorbed moisture, it must be dried with a dehumidified air drying equipment, dew point mini -20°C. Recommended time 2-4hInjection Advice: For unfilled polyamide, Solvay recommends the use of high alloy steel with a weak chromium content. For example: X38CrMoV5-1 (EN Norm) - 1.2367 /1.2343 (DIN Norm). For Mould Temperature, in the case of parts where the surface roughness is required we can recommend a temperature of 90°C to 120°C with an optimum at 105°C. |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 705 CC | RTP Company | HDPE | RTP |
Daelim Po1y® LL-24W | DAELIM INDUSTRIAL CO., LTD. | LLDPE | Daelim Po1y® |
Laprene® 830000823 | SO.F.TER. SPA | SEBS | Laprene® |
KumhoSunny PPO HPP8340 | Shanghai KumhoSunny Plastics Co., Ltd. | PPE+PS | KumhoSunny PPO |
Lion Idemitsu Composites PPS C-140SC | Lion Idemitsu Composites Co., Ltd. | PPS | Lion Idemitsu Composites PPS |