Category: | MPR , Melt Processable Rubber |
Manufacturer: | Advanced Polymer Alloys |
Trademark: | Alcryn® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | bFKL7N_Alcryn-2245-TR.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Alcryn®2245 TR is a melt processable rubber (MPR) material,. This product is available in North America, Europe or Asia Pacific. The processing methods are: blow molding, extrusion, compression molding or injection molding. Alcryn®The main features of 2245 TR are:
Typical application areas include:
|
General Information | |
---|---|
Additive |
|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.06 | g/cm³ | ASTM D792, ISO 1183 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A, 1.91mm, molded) | 47 | ASTM D2240 | |
IRHD Hardness | 47 | ISO 48 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus (1.91mm, molded) | 1.93 | MPa | ASTM D638, ISO 527-2 |
Tensile Strength (yield, 1.91mm, molding) | 6.89 | MPa | ASTM D638, ISO 527-2 |
Tensile Elongation (fracture, 1.91mm, molded) | 420 | % | ASTM D638, ISO 527-2 |
Taber Abrasion Resistance (1000 Cycles, 1000 g, CS-17 Wheel) | 5.00 | mg | ASTM D1044 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Set | 7 | % | ASTM D412 |
Tear Strength 1(24°C) | 19.3 | kN/m | ASTM D624 |
Compression Set | ASTM D395B, ISO 815 | ||
24°C, 22 hr | 15 | % | ASTM D395B, ISO 815 |
100°C, 22 hr | 56 | % | ASTM D395B, ISO 815 |
Clash-Berg Modulus (-61°C) | 68.9 | MPa | ASTM D1043 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Shore Hardness in Air (125°C, 168 hr) | 45 | ISO 188 | |
Change in Ultimate Elongation (125°C, 168 hr) | 450 | % | ASTM D471 |
Change in Durometer Hardness (125°C, 168 hr) | 45 | ASTM D471 | |
Change in Volume | ASTM D471 | ||
24°C, 168 hr, in reference fuel B | 24 | % | ASTM D471 |
100°C, 168 hr, ASTM Standard Oil (No.1) | -39 | % | ASTM D471 |
100°C, 168 hr, ASTM Standard Oil (No.3) | 32 | % | ASTM D471 |
100°C, 168 hr, in water | 7.0 | % | ASTM D471 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature | -91.1 | °C | ASTM D746, ISO 974 |
Additional Information |
---|
The value listed as Density-Specific Gravity, ASTM D792, was tested in accordance with ASTM D471.Torsion Modulus, ASTM D1043, 75°F: 290psiAging Tensile Strength, ASTM D573, 7 days, 257°F: 940psiTorsion Modulus, ASTM D1043, -4°F: 380psiAging 100% Modulus, ASTM D573, 7 days, 257 °F: 240psiAging Elongation At Break, ASTM D573 and ISO 188: 450%Fluid Resistance 7 Days in water, ISO 1817, at 212 °F: 7%Fluid Resistance 7 Days in ASTM Oil no. 1, ISO 1817, at 212 °F: -39%Fluid Resistance 7 Days in IRM 903 Oil no. 3, ISO 1817, at 212 °F: 32%Fluid Resistance 7 Days in ASTM Ref. Fuel no. B, ISO 1817, at 75 °F: 24%Rheological Viscosity, ASTM D3835, 1/300s at 374°F: 115Pa-s |
Injection | Nominal Value | Unit | |
---|---|---|---|
Processing (Melt) Temp | 166 | °C |
Note Message | |
---|---|
1 . | C mould |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Moplen HP740T | PolyMirae | PP Random Copolymer | Moplen |
DESLOY™ DSC901G2 | DESCO Co., Ltd. | PC | DESLOY™ |
3M™ Dyneon™ Fluoroelastomer FX 3735 | 3M Advanced Materials Division | Fluorelastomer | 3M™ Dyneon™ Fluoroelastomer |
Lupoy® 1302-10 | LG Chem Ltd. | PC | Lupoy® |
Sylvin 8205-85UV Brown 7485 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |