| Category: | HDPE , High Density Polyethylene |
| Manufacturer: | Polykemi AB |
| Trademark: | SCANFILL |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | b73PGF_SCANFILL-BOTTLE-BY45C2.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Blow moulding grade |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Uses |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.37 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 0.10 | g/10 min | ISO 1133 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | 20.0 | MPa | ISO 527-2 |
| Tensile Strain (Yield) | 15 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 1800 | MPa | ISO 178 |
| Flexural Stress | 31.0 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179 | ||
| -20°C | 18 | kJ/m² | |
| 23°C | 28 | kJ/m² | |
| Charpy Unnotched Impact Strength | ISO 179 | ||
| -20°C | No Break | ||
| 23°C | No Break |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature 1 | |||
| 0.45 MPa, Unannealed | 85.0 | °C | ISO 75-2/B |
| 1.8 MPa, Unannealed | 42.0 | °C | ISO 75-2/A |
| Vicat Softening Temperature | |||
| -- | 125 | °C | ISO 306/A50 |
| -- | 68.0 | °C | ISO 306/B50 |
| Note Message | |
|---|---|
| 1 . | 120°C/hr |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| VESTOLIT® P 1300 K | VESTOLIT GmbH & Co. KG | PVC, Unspecified | VESTOLIT® |
| TOTAL Polyethylene Lumicene® BM 359 SG | TOTAL Refining & Chemicals | MDPE | TOTAL Polyethylene |
| EverGlide® MB2650 | Polymer Dynamix | SBC | EverGlide® |
| SQUARE® LIM1520-45A/B | Shenzhen SQUARE Silicone Co., Ltd. | Silicone Rubber, LSR | SQUARE® |
| LNP™ LUBRICOMP™ WFL34H compound | SABIC Innovative Plastics | PBT | LNP™ LUBRICOMP™ |