| Category: | PBT , Polybutylene Terephthalate |
| Manufacturer: | PolyOne Corporation |
| Trademark: | Bergadur™ |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | b35g2d_BergadurPB40G15NaturalTMY.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Bergadur™PB40 G15 Natural TM-Y is a polybutene terephthalate (PBT) product, which contains a 15% glass fiber reinforced material. It can be processed by injection molding and is available in Europe. |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| Appearance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.34 | g/cm³ | ISO 1183 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 5000 | MPa | ISO 527-2 |
| Tensile Stress | 85.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 5.0 | % | ISO 527-2 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength (23°C) | 12 | kJ/m² | ISO 179 |
| Charpy Unnotched Impact Strength (23°C) | 60 | kJ/m² | ISO 179 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 110 - 130 | °C | |
| Drying Time | 4.0 - 6.0 | hr | |
| Rear Temperature | 240 - 270 | °C | |
| Middle Temperature | 240 - 270 | °C | |
| Front Temperature | 240 - 270 | °C | |
| Mold Temperature | 75 - 95 | °C |
| Injection instructions |
|---|
| Injection Pressure: MED-HIGHHold Pressure: MED-HIGHScrew Speed: MODERATEBack Pressure: LOW |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Celstran® PA66-AF35-02-US | Celanese Corporation | Nylon 66 | Celstran® |
| Hytrel® 7246 | DuPont Performance Polymers | TPC-ET | Hytrel® |
| Iupilon® N-9 | Mitsubishi Engineering-Plastics Corp | PC | Iupilon® |
| Sylvin 6034-85 Red 6268 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
| MARPOL® FS3 | Marco Polo International, Inc. | PS (EPS) | MARPOL® |