Monprene® MP-2133

Category: TPE , Thermoplastic Elastomer
Manufacturer: Teknor Apex Company
Trademark: Monprene®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: aqG1Er_Monprene-MP-2133.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Monprene®MP-2133 is a thermoplastic elastomer (TPE) material,. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is extrusion or injection molding.

Typical application areas include:
  • Handle
  • safety equipment
  • packing
  • kitchen utensils
  • engineering/industrial accessories
General Information
Uses
  • Safety equipment
  • Handle
  • Packaging
  • Kitchen utensils
  • Washer
  • Pipe fittings
  • Sporting goods
  • Shell
  • Stationery
  • Consumer goods application field
  • Toothbrush handle
  • Medical/nursing supplies
Appearance
  • Opacity
Forms
  • Particle
Processing Method
  • Extrusion
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.03g/cm³ASTM D792
Melt Mass-Flow Rate (MFR) (200°C/5.0 kg)20g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Durometer Hardness ASTM D2240
    Shaw A, 1 sec 47ASTM D2240
    Shaw A, 5 seconds 45ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Stress (300% Strain)2.07MPaASTM D412
Tensile Strength (Break)6.90MPaASTM D412
Tensile Elongation (Break)700%ASTM D412
Compression Set (23°C, 22 hr)25%ASTM D395
InjectionNominal ValueUnit
Rear Temperature 182 - 232°C
Middle Temperature 188 - 238°C
Front Temperature 193 - 243°C
Nozzle Temperature 199 - 249°C
Processing (Melt) Temp 199 - 249°C
Mold Temperature 35.0 - 48.9°C
Injection Pressure 1.38 - 5.52MPa
Injection Rate Fast
Back Pressure 0.172 - 0.689MPa
Screw Speed 50 - 100rpm
Cushion 3.81 - 25.4mm
Injection instructions
Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C).
ExtrusionNominal ValueUnit
Cylinder Zone 1 Temp. 182 - 232°C
Cylinder Zone 2 Temp. 188 - 238°C
Cylinder Zone 3 Temp. 193 - 243°C
Cylinder Zone 5 Temp. 199 - 249°C
Die Temperature 199 - 249°C
Extrusion instructions
Screw Speed: 30 to 100 rpm
Resin Grade Manufacturer Category Trademark
Rilsan® BECV0 P40 TL Arkema Nylon 11 Rilsan®
Ad-Tech Epoxy EL-318 Ad-Tech Plastic Systems Corp. Epoxy Ad-Tech Epoxy
Hydrin® H45 Zeon Chemicals L.P. Epoxy Hydrin®
Lion Idemitsu Composites PPS G142Z1 Lion Idemitsu Composites Co., Ltd. PPS Lion Idemitsu Composites PPS
Kinta FR3600A Kinta Technology (Hong Kong) Co., Ltd. ABS Kinta