Category: | HDPE, UHMW , High Density Polyethylene Resin |
Manufacturer: | ExxonMobil Chemical |
Trademark: | ExxonMobil™ HDPE |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | aQgPrq_ExxonMobil-HDPE-HD-7960-13.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
HD 7960.13 is a high molecular weight high density polyethylene blown film resin. The film made of HD 7960.13 has excellent impact resistance, toughness and stiffness. HD 7960.13 is especially recommended for films with a thickness of less than 0.5 mils. |
General Information |
---|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Melt Mass-Flow Rate (MFR) (190°C/21.6 kg) | 10 | g/10 min | ASTM D1238 |
Films | Nominal Value | Unit | Test Method |
---|---|---|---|
secant modulus | ASTM D882 | ||
1% secant, MD | 1060 | MPa | ASTM D882 |
1% secant, TD | 1130 | MPa | ASTM D882 |
Tensile Strength | ASTM D882 | ||
MD : Yield | 37.9 | MPa | ASTM D882 |
TD : Yield | 32.9 | MPa | ASTM D882 |
MD : Fracture | 84.1 | MPa | ASTM D882 |
TD : Fracture | 71.3 | MPa | ASTM D882 |
Tensile Elongation | ASTM D882 | ||
MD : Fracture | 270 | % | ASTM D882 |
TD : Fracture | 380 | % | ASTM D882 |
Dart Drop Impact | 300 | g | ASTM D1709A |
Elmendorf Tear Strength | ASTM D1922 | ||
MD | 7.0 | g | ASTM D1922 |
TD | 32 | g | ASTM D1922 |
Legal statement |
---|
有关潜在食品接触应用合规信息(例如:FDA、EU、HPFB),请与埃克森美孚化工客户服务代表联系。本产品不宜在医疗应用中使用,亦不应在任何此类应用中使用 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
MarFlex® 9656 | Chevron Phillips Chemical Company LLC | HDPE | MarFlex® |
Novodur® H605 | Styrolution | ABS | Novodur® |
Badaprene® TPV 55A 1049 | Bada AG | PP+EPDM | Badaprene® |
Bergadur™ PB400 G/C 30 U BK075 | PolyOne Corporation | PBT | Bergadur™ |
Argothane® SS-1495SL-95 | Argotec LLC | TPU, Unspecified | Argothane® |