Category: | ABS , Acrylonitrile Butadiene Styrene |
Manufacturer: | Polykemi AB |
Trademark: | POLYabs |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | ZiEw9M_POLYabs-V0E.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Flame retardant |
General Information | |
---|---|
Additive |
|
Features |
|
UL File Number |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.20 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/5.0 kg) | 15 | g/10 min | ISO 1133 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow | 0.50 to 0.70 | % | |
Flow | 0.50 to 0.70 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | 40.0 | MPa | ISO 527-2 |
Tensile Strain (Yield) | 6.0 | % | ISO 527-2 |
Flexural Modulus (23°C) | 2000 | MPa | ISO 178 |
Flexural Stress | 70.0 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | ||
-20°C | 8.0 | kJ/m² | |
23°C | 18 | kJ/m² |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature 1 | |||
0.45 MPa, Unannealed | 83.0 | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 73.0 | °C | ISO 75-2/A |
Vicat Softening Temperature | 90.0 | °C | ISO 306/B50 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (1.60 mm) | V-0 | UL 94 | |
Glow Wire Ignition Temperature (2.00 mm) | 960 | °C | IEC 60695-2-13 |
Note Message | |
---|---|
1 . | 120°C/hr |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
PRL NY66-GP1-(color)H | Polymer Resources Ltd. | Nylon 66 | PRL |
Sindustris PP GP1008FE | Sincerity Australia Pty Ltd. | PP, Unspecified | Sindustris PP |
Eltex® A4040 | INEOS Olefins & Polymers Europe | MDPE | Eltex® |
PETOPLEN MH 180 | PETKIM Petrokimya Holding A.S. | PP, Unspecified | PETOPLEN |
Sarlink® TPE ML-1680N NAT (PRELIMINARY DATA) | Teknor Apex Company | TPE | Sarlink® TPE |