Category: | PPS , Polyphenylene Sulfide |
Manufacturer: | Bada AG |
Trademark: | Badatron® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | ZAXonp_BadatronPPSGFM65.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
65% glass fibres reinforced and mineral filled injection moulding grade |
General Information | |
---|---|
Filler / Reinforcement |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density (23°C) | 2.03 | g/cm³ | ISO 1183 |
Water Absorption (Saturation, 23°C) | 0.020 | % | ISO 62 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus (23°C) | 17000 | MPa | ISO 527-2/1 |
Tensile Stress (Break, 23°C) | 115 | MPa | ISO 527-2/5 |
Tensile Strain (Break, 23°C) | 1.0 | % | ISO 527-2/5 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength 1(23°C) | 5.0 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength 2(23°C) | 15 | kJ/m² | ISO 179/1eU |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating | UL 94 | ||
0.8 mm | V-0 | UL 94 | |
1.6 mm | V-0 | UL 94 | |
Glow Wire Flammability Index (1.6 mm) | 960 | °C | IEC 60695-2-12 |
Glow Wire Ignition Temperature (1.6 mm) | 960 | °C | IEC 60695-2-13 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 140 | °C | |
Drying Time | 3.0 - 4.0 | hr | |
Processing (Melt) Temp | 300 - 340 | °C | |
Mold Temperature | 140 - 180 | °C |
Note Message | |
---|---|
1 . | 80x10x4 mm |
2 . | 80x10x4 mm |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
MarFlex® 7114 | Chevron Phillips Chemical Company LLC | LLDPE | MarFlex® |
HiFill® PA6/6 GB20 L | Techmer Engineered Solutions | Nylon 66 | HiFill® |
Pibiflex® RFB40011 NERO | SO.F.TER. SPA | TPC-ET | Pibiflex® |
Sumiliteresin® PR-53123 | SBHPP | Phenolic | Sumiliteresin® |
Moplen EP545L | LyondellBasell Industries | PP Copolymer | Moplen |