Plaslube® AC-80/TF/20

Category: Acetal (POM) Copolymer , Acetal (POM) Copolymer
Manufacturer: Techmer Engineered Solutions
Trademark: Plaslube®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: YvBUu2_Plaslube-AC-80-TF-20.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Plaslube®AC-80/TF/20 is a polyoxymethylene (POM) copolymer product,. It can be processed by injection molding and is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. Typical application areas are: engineering/industrial accessories.

Features include:
  • flame retardant/rated flame
  • ROHS certification
  • Copolymer
  • Lubrication
General Information
Additive
  • PTFE lubricant (20%)
Features
  • Copolymer
  • Lubrication
Uses
  • Gear
  • Bearing
RoHS Compliance
  • RoHS compliance
Forms
  • Particle
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.51g/cm³ASTM D792
Molding Shrinkage - Flow (3.18 mm)2.0%ASTM D955
Water Absorption (24 hr)0.23%ASTM D570
MechanicalNominal ValueUnitTest Method
Tensile Strength (23°C)41.4MPaASTM D638
Flexural Modulus (23°C)2140MPaASTM D790
Flexural Strength (23°C)64.1MPaASTM D790
Coefficient of Friction ASTM D1894
    With steel-dynamic 0.15ASTM D1894
    With steel-static 0.070ASTM D1894
ImpactNominal ValueUnitTest Method
Notched Izod Impact (23°C, 3.18 mm)48J/mASTM D256
ThermalNominal ValueUnitTest Method
Deflection Temperature Under Load (1.8 MPa, Unannealed)100°CASTM D648
FlammabilityNominal ValueTest Method
Flame Rating (1.59 mm)HBUL 94
Additional Information
Coefficient of Friction, Static, Thrust washer, 40psi, ambient temp.: 0.07Coefficient of Friction, Dynamic, Thrust washer, 40psi, 50 ft/min, ambient temp.: 0.15Limiting PV, Thrust washer, 100 FPM, ambient temp.: 1.3E4
InjectionNominal ValueUnit
Drying Temperature 82.2°C
Drying Time 1.0 - 2.0hr
Suggested Max Moisture 0.20%
Rear Temperature 177 - 188°C
Middle Temperature 188 - 199°C
Front Temperature 182 - 193°C
Nozzle Temperature 177 - 188°C
Processing (Melt) Temp 188 - 204°C
Mold Temperature 76.7 - 93.3°C
Injection Rate Moderate-Fast
Back Pressure 0.345 - 0.689MPa
Injection instructions
Screw Speed: MediumRecommendations for Molding and Tool Conditions: Well ventedMoisture Content, as received: Product is packaged at 0.2% or less.Drying not normally required. Dry at 180°F for 1 to 2 hours if necessary.
Resin Grade Manufacturer Category Trademark
Prixene® EA200I54 POLYMAT HDPE Prixene®
Sumikon® EME-7320AR Sumitomo Bakelite Co., Ltd. Epoxy Sumikon®
Sylvin 5201-80 Natural Sylvin Technologies Incorporated PVC, Unspecified Sylvin
Keltan® 5470C LANXESS Buna GmbH EPDM Keltan®
Kazan LDPE 15813-020 OKP 22 1111 3201 Kazanorgsintez Joint Stock Company LDPE Kazan LDPE