Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | Polykemi AB |
Trademark: | SCANAMID 6 |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | YBAz33_SCANAMID-6-B22-E-F20.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Glass fibre-reinforced, Modified |
General Information | |
---|---|
Filler / Reinforcement |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.27 | -- | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | |||
Across Flow | 0.90 | -- | % | |
Flow | 0.40 | -- | % |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Stress | 130 | 100 | MPa | ISO 527-2 |
Tensile Strain (Break) | 4.0 | 7.0 | % | ISO 527-2 |
Flexural Modulus (23°C) | 6400 | 4000 | MPa | ISO 178 |
Flexural Stress | 200 | 130 | MPa | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength (23°C) | 12 | 16 | kJ/m² | ISO 179 |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature 1 | ||||
0.45 MPa, Unannealed | 210 | -- | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 190 | -- | °C | ISO 75-2/A |
Vicat Softening Temperature | 200 | -- | °C | ISO 306/B50 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flame Rating (1.60 mm) | HB | -- | UL 94 | |
Glow Wire Ignition Temperature (2.00 mm) | 650 | -- | °C | IEC 60695-2-13 |
Note Message | |
---|---|
1 . | 120°C/hr |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
New-prene™ 7155 | Total Polymer Vision (Suzhou) Co., LTD | PP+EPDM | New-prene™ |
Akulon® S223-HM8 | DSM Engineering Plastics | Nylon 66 | Akulon® |
APEX® 1526 | Teknor Apex Company | PVC, Flexible | APEX® |
HI-ZEX™ 6800S | Prime Polymer Co., Ltd. | HDPE | HI-ZEX™ |
Kostil® B 366 | Versalis S.p.A. | SAN | Kostil® |