| Category: | TPE , Thermoplastic Elastomer |
| Manufacturer: | Mitsubishi Chemical Performance Polymers, Inc. |
| Trademark: | THERMORUN® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | Y8Bo7v_THERMORUN-3855B-N.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| THERMORUN®3855B/N is a thermoplastic elastomer (TPE) material,. This product is available in North America, Europe or Asia Pacific. The processing method is extrusion or injection molding. THERMORUN®The main characteristics of 3855B/N are: low hardness. |
| General Information | |
|---|---|
| Features |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.890 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (230°C/5.0 kg) | 12 | g/10 min | ISO 1133 |
| Molding Shrinkage | ISO 294-4 | ||
| Vertical flow direction | 1.5 - 2.0 | % | ISO 294-4 |
| Flow direction | 1.5 - 2.0 | % | ISO 294-4 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 83 | ISO 868 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ISO 37 | ||
| 100% strain | 4.00 | MPa | ISO 37 |
| 300% strain | 5.20 | MPa | ISO 37 |
| Tensile Stress (Break) | 12.0 | MPa | ISO 37 |
| Tensile Elongation (Break) | 710 | % | ISO 37 |
| Tear Strength | 51 | kN/m | ISO 34-1 |
| Compression Set (70°C, 22 hr) | 47 | % | ISO 815 |
| Additional Information |
|---|
| Data obtained using JIS test methods. |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Wellamid® NY1599-BK11 | Wellman Engineering Resins | Nylon 66 | Wellamid® |
| Unichem 4075 | Colorite Polymers | PVC, Unspecified | Unichem |
| Buna® EP G 5567 | LANXESS Corporation | EPDM | Buna® EP |
| LNP™ THERMOCOMP™ 9X99089 compound | SABIC Innovative Plastics Europe | PEI | LNP™ THERMOCOMP™ |
| LUVOCOM® 3-8437/BL | Lehmann & Voss & Co. | Nylon 6 | LUVOCOM® |