Elastollan® C75AW is a polyester-based thermoplastic polyurethane (TPU) containing a plasticizer. It exhibits excellent abrasion resistance and toughness, good hydrolytic stability, good heat, oil, fuel and solvent resistance. It has excellent damping characteristics and outstanding resistance to tear propagation. Elastollan® C75AW is supplied uncolored in pellet form. |
General Information | |
---|---|
Features |
|
Appearance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.17 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A) | 74 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus (Injection Molded) | 20.7 | MPa | ASTM D412 |
Flexural Modulus (Injection Molded) | 10.3 | MPa | ASTM D790 |
Taber Abrasion Resistance | 40.0 | mg | ASTM D1044 |
Abrasion - DIN | 10 | mm³ | DIN 53516 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Softening Point - DMA | 100 | °C | Internal Method |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ASTM D412 | ||
100% Strain | 5.17 | MPa | |
300% Strain | 11.0 | MPa | |
Tensile Strength | 28.3 | MPa | ASTM D412 |
Tensile Elongation (Break) | 710 | % | ASTM D412 |
Tear Strength 1 | 82.3 | kN/m | ASTM D624 |
Compression Set | ASTM D395B | ||
23°C, 22 hr | 25 | % | |
70°C, 22 hr | 40 | % |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Glass Transition Temperature | -46.0 | °C | Internal Method |
Vicat Softening Temperature | 77.0 | °C | ASTM D1525 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Suggested Max Moisture | 0.030 | % | |
Rear Temperature | 170 to 210 | °C | |
Middle Temperature | 170 to 210 | °C | |
Front Temperature | 170 to 210 | °C | |
Nozzle Temperature | 200 to 210 | °C |
Note Message | |
---|---|
1 . | Die C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
SLOVAMID® 6 NG GF 45 SGF | Plastcom | Nylon 6 | SLOVAMID® 6 |
Bashplast Compound SSP-A17 (BP)/CB-B25 (BP) | Bashplast Ltd. | PE, Unspecified | Bashplast Compound |