| Category: | PP, Unspecified , Polypropylene |
| Manufacturer: | TBA Electro Conductive Products Ltd. |
| Trademark: | ECP |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | Y23qvh_ECP-115.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
A wide range of polymer bases are employed to produce conductive plastics, including the polyolefines, nylons and ABS.Typical applications are illustrated using ECP 104 mineral filled conductive polypropylene which can be used to mould a variety of containers for static sensitive devices and PCB handling equipment. The mineral filler produces rigid mouldings with excellent dimensional stability.
|
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | |
|---|---|---|---|
| Density | 1.04 | g/cm³ | |
| Melt Mass-Flow Rate (MFR) | |||
| 230°C/10.0 kg | 10 | g/10 min | |
| 230°C/5.0 kg | 1.0 | g/10 min |
| Mechanical | Nominal Value | Unit | |
|---|---|---|---|
| Tensile Modulus | 1300 | MPa | |
| Tensile Stress | 20.0 | MPa | |
| Flexural Modulus | 1200 | MPa | |
| Flexural Stress | 29.0 | MPa |
| Impact | Nominal Value | Unit | |
|---|---|---|---|
| Charpy Notched Impact Strength | 5.0 | kJ/m² | |
| Charpy Unnotched Impact Strength | No Break |
| Thermal | Nominal Value | Unit | |
|---|---|---|---|
| Heat Deflection Temperature | |||
| 0.45 MPa, Unannealed | 69.0 | °C | |
| 1.8 MPa, Unannealed | 46.0 | °C |
| Electrical | Nominal Value | Unit | |
|---|---|---|---|
| Surface Resistivity | 1.0E+4 | ohms |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Rulon® J | Saint Gobain Performance Plastics | PTFE | Rulon® |
| QAMAR FD18N | SPDC Ltd. | LLDPE | QAMAR |
| SAMAT EP5001C(f1) | POLYROCKS CHEMICAL CO., LTD | PP, Unspecified | SAMAT |
| Topolymer® 5711-851M | Dongguan Top Polymer Enterprise | TPE | Topolymer® |
| LG EVA EC15006 | LG Chem Ltd. | EVA | LG EVA |