Sulphur cured Ethylene Propylene Terpolymer 60-70 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated in accordance with BS2494 Type ‘W'. For joint rings, sealing rings and gaskets, and general applications where water and weathering resistance is required |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
Hardness | Nominal Value | Test Method | |
---|---|---|---|
IRHD Hardness | 65 | ASTM D1415, ISO 48 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength (Yield) | 11.0 | MPa | ASTM D412, ISO 37 |
Tensile Elongation (Break) | 450 | % | ASTM D412, ISO 37 |
Compression Set | |||
70°C, 22 hr | 14 | % | ASTM D395B |
70°C, 22 hr 1 | 14 | % | ISO 815 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Strength in Air (168°C, 70 hr) | -20 | % | ASTM D412, ISO 37 |
Change in Ultimate Elongation in Air (168°C, 70 hr) | -30 | % | ASTM D412, ISO 37 |
Change in IRHD Hardness in Air (168°C, 70 hr) | 5.0 | ASTM D573, ISO 188 |
Thermal | Nominal Value | Unit | |
---|---|---|---|
Maximum Operating Temperature | 150 | °C |
Additional Information |
---|
Minimum Operating Temperature: -30°C (-22°F) |
Note Message | |
---|---|
1 . | Type B |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
DOMAMID® 66B40 | DOMO Engineering Plastics SPA | Nylon 66 | DOMAMID® |
Elastron® V P.V101.A90.N | Elastron USA, Inc. | TPV | Elastron® V |
EnviroPro 2014TF20 | West Michigan Compounding | PP Copolymer | EnviroPro |
Optix® CA-927 G | Plaskolite West, Inc. | Acrylic (PMMA) | Optix® |
Adsyl 7415 XCP | LyondellBasell Industries | Polyolefin, Unspecified | Adsyl |