Wellamid® GSF25/15-66 22L-NBK1 is a Polyamide 66 (Nylon 66) material filled with 40% glass bead\glass fiber. It is available in Asia Pacific, Europe, Latin America, or North America. Typical application of Wellamid® GSF25/15-66 22L-NBK1: Automotive |
General Information | |
---|---|
Filler / Reinforcement |
|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.45 | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow : 23°C | 1.1 to 1.5 | % | |
Flow : 23°C | 0.50 to 0.90 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Yield, 23°C) | 115 | MPa | ISO 527-2 |
Tensile Strain (Yield, 23°C) | 3.0 | % | ISO 527-2 |
Flexural Modulus (23°C) | 7300 | MPa | ISO 178 |
Flexural Stress (23°C) | 175 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact Strength (23°C) | 3.0 | kJ/m² | ISO 180 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 235 | °C | ISO 75-2/A |
Melting Temperature (DSC) | 260 | °C | ISO 3146 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
megol® DP2339 85 | API SpA | SEBS | megol® |
Nypol® PA A3 G27 NTLA010 NR364 MSM | Petropol Industry and Trade of Polymers LTDA | Nylon 66 | Nypol® PA |
Chemlon® 125 GVH | Teknor Apex Company (Chem Polymer) | Nylon 66 | Chemlon® |
Geon™ Vinyl Rigid Extrusion 87624 | PolyOne Corporation | PVC, Rigid | Geon™ Vinyl Rigid Extrusion |
NILAMID® XT6 GF30 | Nilit Plastics | PPA | NILAMID® |